Electrical and Structural Properties of MeV Si+ Ion Implantation in Silicon
Published online by Cambridge University Press: 26 February 2011
Abstract
The electrical properties of residual MeV ion implantation damage in Si after annealing from 600 to 1100°C for 1 hour have been investigated using Deep Level Transient Spectroscopy, Capaciatance-Voltage, and Current-Voltage measurements. These data have been correlated with structural defects imaged by Transmission Electron Microscopy. It is shown that at least 4 deep levels are associated with the buried layer of extended defects after annealing at 800, 900, 1000 and 1100°C. Additionally, for the wafer annealed at 800°C at least 5 more deep level centers are present in the device layer above the buried defects.