Published online by Cambridge University Press: 25 February 2011
Measurements of the electrical conductivity, Seebeck coefficient and Hall mobility from -300 K to -1300 K have been carried out on multiphase hotpressed samples of the nominal composition B6Si. In all samples the conductivity and the p-type Seebeck coefficient both increase smoothly with increasing temperature. By themselves, these facts suggest small-polaronic hopping between inequivalent sites. The measured Hall mobilities are always low, but vary in sign. A possible explanation is offered for this anomalous behavior.