Hostname: page-component-78c5997874-v9fdk Total loading time: 0 Render date: 2024-11-19T09:31:08.389Z Has data issue: false hasContentIssue false

Wear and Adhesion of thin Carbon Coatings

Published online by Cambridge University Press:  21 February 2011

Hsin-Fu Wang
Affiliation:
Department of Materials Science and Engineering, University of Florida, Gainesville, FL 32611.
John C. Nelson
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455.
Chien-Li Lin
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455.
Joel W. Hoehn
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455.
William W. Gerberich
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455.
Get access

Abstract

The ability of a hard coating to resist delamination in wear applications is found to depend on the substrate crystal orientation. A variety of alloys with and without a carbon coating were tested by microscratching with a diamond stylus. The hardness of the carbon coating was characterized by nanoindentation techniques before the microscratch tests. As the diamond passed from one crystal to another differing amounts of damage were observed for each crystal orientation. The width of the delaminated region was found to be dependent on the extent of the slip line fields in the substrate generated by the scratching. To eliminate the possibility of differing adhesion on different crystal faces, a nickel aluminide intermetallic with the two crystals rotated about the same pole was tested. In the uncoated state when scratched across the grain boundary the slip line fields were extensive for one crystal but limited for the other crystal. Similar fixed-load scratches on the carbon coating produced delamination on the easy slip orientation but only a slight deformation of the coating on the other crystal. The observed failure appears to be due to the deformation of the substrate and not inferior adhesion of the coating to the crystal face. This finding should have important ramifications in the design and failure analysis of systems, such as magnetic recording media, medical implants, etc.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Sioshanshi, P., Orthopaedics Today, 11, August (1991).Google Scholar
2. Poggie, R.A., Mishra, A.K., Davidson, J.A. and Wert, J.J., Surface Modification Technology VI, ed Sudarshan, T.S. and Braza, J.F. (TMS Proceedings, PA, 1992), p. 323.Google Scholar
3. Akiyama, S., Nakagawa, S. and Naoe, M., IEEE Trans. Magn, 27, 4751 (1991).Google Scholar
4. Grill, A., Wear, 168, 143 (1993).Google Scholar
5. Pharr, G.M., Oliver, W.C. and Brotzen, F.R., J. Mater. Res, 7, 613 (1992).Google Scholar
6. Oliver, W.C. and Pharr, G.M., J. Mater. Res, 7, 1564 (1992).Google Scholar
7. Kadijk, S.E. and Van Groenou, A.B., Wear, 139, 115 (1990).Google Scholar
8. Suh, N.P., Tribophysics , Chater 4.Google Scholar