2-Dimensional Controlled Large Lateral Grain Growth on the Floating Amorphous Silicon Film by Excimer Laser Recrystallization

Published online by Cambridge University Press:  01 February 2011

In-Hyuk Song
Affiliation:
School of Electrical Engineering, Seoul National University, Seoul 151-742, Korea Phone: +82-2-880-7992, Fax: +82-2-883-0827, E-mail:ihsong@emlab.snu.ac.kr
Su-Hyuk Kang
Affiliation:
School of Electrical Engineering, Seoul National University, Seoul 151-742, Korea Phone: +82-2-880-7992, Fax: +82-2-883-0827, E-mail:ihsong@emlab.snu.ac.kr
Woo-Jin Nam
Affiliation:
School of Electrical Engineering, Seoul National University, Seoul 151-742, Korea Phone: +82-2-880-7992, Fax: +82-2-883-0827, E-mail:ihsong@emlab.snu.ac.kr
Min-Koo Han
Affiliation:
School of Electrical Engineering, Seoul National University, Seoul 151-742, Korea Phone: +82-2-880-7992, Fax: +82-2-883-0827, E-mail:ihsong@emlab.snu.ac.kr
Get access

Abstract

We have successfully obtained large lateral grains with well-controlled grain boundary. The proposed excimer laser annealing (ELA) method produces 2-dimensionally controlled grain growth because the temperature gradient is induced in two directions. Along the channel direction, the floating active structure produces large thermal gradient due to very low thermal conductivity of the air-gap. Along the perpendicular direction to the channel, the surface tension effect also produces thermal gradient. The proposed ELA method can control the grain boundary perpendicular and parallel to current path with only one laser irradiation.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Crowder, M. A., Carey, P. G., Smith, P. M., Sposili, R.S., Cho, H. S. and Im, J.S., IEEE Electron Device Letter, Vol. 19, p. 306, 1998.Google Scholar
[2] Oh, C. H. and Matsumura, M., IEEE Electron Device Letter, Vol. 22, p. 20, 2001.Google Scholar
[3] Jeon, J. H., Lee, M.C., Park, K. C., Jung, S.H. and Han, M. K., IEDM Tech. Digest, p.213, 2000.Google Scholar
[4] Kim, C. H., Song, I. H., Jung, S. H. and Han, M. K., IEDM Tech. Digest, p 751, 2001 Google Scholar
[5] Im, J.S., and Kim, H.J., Appl. Phys. Lett., Vol. 63, no. 14, p. 1969, 1993.Google Scholar
[6] Giust, G. K. and Sigmon, T. W., J. Appl. Phys., vol. 81, No.3, p. 1204, 1997 Google Scholar