Hostname: page-component-99c86f546-45s75 Total loading time: 0.342 Render date: 2021-11-28T02:27:18.648Z Has data issue: true Feature Flags: { "shouldUseShareProductTool": true, "shouldUseHypothesis": true, "isUnsiloEnabled": true, "metricsAbstractViews": false, "figures": true, "newCiteModal": false, "newCitedByModal": true, "newEcommerce": true, "newUsageEvents": true }

Study on the tensile and wear properties of laser-cladded IN718 superalloy reinforced by carbon nanoproducts transformed from carbon nanotubes

Published online by Cambridge University Press:  02 October 2020

Zhijun Chen
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China
Yuan Chen*
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China Mechanical & Electrical Engineering College, Jinhua Polytechnic, Jinhua 321017, P.R. China
Qin Zhang
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China
Zhehe Yao
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China
Qunli Zhang
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China
Liang Wang
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China
Jianhua Yao
Affiliation:
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, P.R. China
Xiaobo Wang
Affiliation:
Beijing Aerospace Xinfeng Machinery Equipment Co., Ltd., Beijing 100854, P.R. China
*
a)Address all correspondence to this author. e-mail: 20191044@jhc.edu.cn
Get access

Abstract

Nickel-coated carbon nanotubes (Ni-CNTs) were achieved by electroless plating. Laser cladded IN718 and IN718 with 10, 30, and 50 wt% additions of Ni-CNTs were fabricated. The structural evolution of CNTs in the laser-deposited layers was studied; the microstructure, tensile, and wear properties of the laser-cladded alloys were characterized. The results show that CNTs in the laser-deposited layers are mostly transformed to carbon nanoproducts (CNPs) in the forms of graphene nanosheets, graphene fragments, carbon nanoribbons, and diamond-like nanoparticles by unzipping, interbonding, collapsing, and curvature of CNTs. The interdendritic Laves phase formation is dramatically depressed due to the addition of Ni-CNTs, but the excess addition of the Ni-CNTs can undesirably increase the formation of NbC. The addition of Ni-CNTs effectively improves the tensile and wear properties. The most superior tensile and wear properties are achieved in the layers with 30 and 50 wt% additions of Ni-CNTs, respectively. The generation of intermetallic phase and CNPs are revealed to be two dominant effects both on the tensile and wear properties of the laser-cladded alloys.

Type
Article
Copyright
Copyright © The Author(s), 2020, published on behalf of Materials Research Society by Cambridge University Press

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Zhang, Y.N., Cao, X., Wanjara, P., and Medraj, M.: Tensile properties of laser additive manufactured Inconel 718 using filler wire. J. Mater. Res. 29, 20062020 (2014).CrossRefGoogle Scholar
Liu, Z.Y. and Qi, H.: Effects of substrate crystallographic orientations on crystal growth and microstructure formation in laser powder deposition of nickel-based superalloy. Acta Mater. 87, 248258 (2015).CrossRefGoogle Scholar
Rolink, G., Vogt, S., Senčekova, L., Weisheit, A., Poprawe, R., and Palm, M.: Laser metal deposition and selective laser melting of Fe-28 at.% Al. J. Mater. Res. 29, 20362043 (2014).CrossRefGoogle Scholar
Bi, G., Ng, G.K.L., Teh, K.M., and Jarfors, A.E.W.: Feasibility study on the laser aided additive manufacturing of die inserts for liquid forging. Mater. Des. 31, S112S116 (2010).CrossRefGoogle Scholar
Sui, S., Chen, J., Zhang, R., Ming, X.L., Liu, F.C., and Lin, X.: The tensile deformation behavior of laser repaired Inconel 718 with a non-uniform microstructure. Mater. Sci. Eng. A-Struct. 688, 480487 (2017).CrossRefGoogle Scholar
Qi, H., Azer, M. and Singh, P.: Adaptive toolpath deposition method for laser net shape manufacturing and repair of turbine compressor airfoils. Int. J. Adv. Manuf. Technol. 48, 121131 (2010).CrossRefGoogle Scholar
Mantrala, K.M., Das, M., Balla, V.K., Srinivasa Rao, C., and Kesava Rao, V.V.S.: Laser-deposited CoCrMo alloy: Microstructure, wear, and electrochemical properties. J. Mater. Res. 29, 20212027 (2014).CrossRefGoogle Scholar
Yao, J.H., Ding, Y.P., Liu, R., Zhang, Q.L., and Wang, L.: Wear and corrosion performance of laser-clad low-carbon high-molybdenum stellite alloys. Opt. Laser Technol. 107, 3245 (2018).CrossRefGoogle Scholar
Iijima, S.: Helical microtubules of graphitic carbon. Nature 354, 5658 (1991).CrossRefGoogle Scholar
Treacy, M.M.J., Ebbesen, T.W., and Gibson, J.M.: Exceptionally high Young's modulus observed for individual carbon nanotubes. Nature 381, 678680 (1996).CrossRefGoogle Scholar
Wong, E.W., Sheehan, P.E., and Lieber, C.M.: Nanobeam mechanics: Elasticity, strength, and toughness of nanorods and nanotubes. Science 277, 1971 (1997).CrossRefGoogle Scholar
Peng, B., Locascio, M., Zapol, P., Li, S., Mielke, S.L., Schatz, G.C., and Espinosa, H.D.: Measurements of near-ultimate strength for multiwalled carbon nanotubes and irradiation-induced crosslinking improvements. Nat. Nanotechnol. 3, 626631 (2008).CrossRefGoogle ScholarPubMed
Yakobson, B.I., Brabec, C.J., and Bernholc, J.: Nanomechanics of carbon tubes: Instabilities beyond linear response. Phys. Rev. Lett. 76, 25112514 (1996).CrossRefGoogle ScholarPubMed
Yan, H. and Qiu, H.X.: Fabrication of carbon nanotube reinforced A356 nanocomposites. J. Mater. Res. 31, 22772283 (2016).CrossRefGoogle Scholar
Yuan, C., Tan, Z.Q., Fan, G.L., Chen, M.L., Zheng, Q., and Li, Z.G.: Fabrication and mechanical properties of CNT/Al composites via shift-speed ball milling and hot-rolling. J. Mater. Res. 34, 26092619 (2019).CrossRefGoogle Scholar
Jiang, L.Y., Liu, T.T., Zhang, C.D., Zhang, K., Li, M.C., Ma, T., and Liao, W.H.: Preparation and mechanical properties of CNTs-AlSi10Mg composite fabricated via selective laser melting. Mater. Sci. Eng.-A Struct. 734, 171177 (2018).CrossRefGoogle Scholar
Gu, D.D., Rao, X.W., Dai, D.H., Ma, C.L., Xi, L.X., and Lin, K.J.: Laser additive manufacturing of carbon nanotubes (CNTs) reinforced aluminum matrix nanocomposites: Processing optimization, microstructure evolution and mechanical properties. Addit. Manuf. 29, 100801 (2019).Google Scholar
Hwang, J.Y., Neira, A., Scharf, T.W., Tiley, J., and Banerjee, R.: Laser-deposited carbon nanotube reinforced nickel matrix composites. Scr. Mater. 59, 487490 (2008).CrossRefGoogle Scholar
Wang, P., Zhang, B.C., Tan, C.C., Raghavan, S., Lim, Y.F., Sun, C.N., Wei, J., and Chi, D.Z.: Microstructural characteristics and mechanical properties of carbon nanotube reinforced Inconel 625 parts fabricated by selective laser melting. Mater. Des. 112, 290299 (2016).CrossRefGoogle Scholar
Zhang, B.C., Bi, G.J., Chew, Y.X., Wang, P., Ma, G.Y., Liu, Y.F., and Moon, S.K.: Comparison of carbon-based reinforcement on laser aided additive manufacturing Inconel 625 composites. Appl. Surf. Sci. 490, 522534 (2019).CrossRefGoogle Scholar
Song, X.L., Lei, J.B., Xie, J.C., and Fang, Y.: Microstructure and electrochemical corrosion properties of nickel-plated carbon nanotubes composite Inconel718 alloy coatings by laser melting deposition. Opt. Laser Technol. 119, 105593 (2019).CrossRefGoogle Scholar
Chen, Y., Lu, F.G., Zhang, K., Nie, P.L., Elmi Hosseini, S.R., Feng, K., and Li, Z.G.: Laser powder deposition of carbon nanotube reinforced nickel-based superalloy Inconel 718. Carbon 107, 361370 (2016).CrossRefGoogle Scholar
Chen, Y., Zhang, Q., Chen, Z.J., Wang, L., Yao, J.H., and Kovalenko, V.: Study on the element segregation and Laves phase formation in the carbon nanotubes reinforced IN718 superalloy by laser cladding. Powder Technol. 355, 163171 (2019).CrossRefGoogle Scholar
Vishwakarma, K.R., Richards, N.L., and Chaturvedi, M.C.: Microstructural analysis of fusion and heat affected zones in electron beam welded ALLVAC® 718PLUS™ superalloy. Mater. Sci. Eng. A-Struct. 480, 517528 (2008).CrossRefGoogle Scholar
DuPont, J.N., Marder, A.R., Notis, M.R., and Robino, C.V.: Solidification of Nb-bearing superalloys: Part II. Pseudoternary solidification surfaces. Metall. Mater. Trans. A 29, 27972806 (1998).CrossRefGoogle Scholar
Zhang, Y.C., Li, Z.G., Nie, P.L., and Wu, Y.X.: Carbide and nitride precipitation during laser cladding of Inconel 718 alloy coatings. Opt. Laser Technol. 52, 3036 (2013).CrossRefGoogle Scholar
Bang, S.Y., Ryu, J.H., Choi, B.G., and Shim, K.B.: A simple route for fabrication of graphene nanoribbons by pulsed laser irradiation in ethanol. J. Alloys Compd. 618, 3336 (2015).CrossRefGoogle Scholar
Ma, R.Z., Wei, B.Q., Xu, C.L., Liang, J., and Wu, D.H.: The morphology changes of carbon nanotubes under laser irradiation. Carbon 38, 623641 (2000).CrossRefGoogle Scholar
Sun, L.T., Gong, J.L., Zhu, Z.Y., Zhu, D.Z., Wang, Z.X., Zhang, W., Hu, J.G., and Li, Q.T.: Synthesis and characterization of diamond nanowires from carbon nanotubes. Diam. Relat. Mater. 14, 749752 (2005).CrossRefGoogle Scholar
Zhang, F.M., Shen, J., Sun, J.F., Zhu, Y.Q., Wang, G., and McCartney, G.: Conversion of carbon nanotubes to diamond by spark plasma sintering. Carbon 43, 12541258 (2005).CrossRefGoogle Scholar
Chen, Y., Guo, Y.B., Xu, M.J., Ma, C.F., Zhang, Q., Wang, L., Yao, J.H., and Li, Z.G.: Study on the element segregation and Laves phase formation in the laser metal deposited IN718 superalloy by flat top laser and gaussian distribution laser. Mater. Sci. Eng. A-Struct. 754, 339347 (2019).CrossRefGoogle Scholar

Send article to Kindle

To send this article to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about sending to your Kindle. Find out more about sending to your Kindle.

Note you can select to send to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be sent to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Study on the tensile and wear properties of laser-cladded IN718 superalloy reinforced by carbon nanoproducts transformed from carbon nanotubes
Available formats
×

Send article to Dropbox

To send this article to your Dropbox account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Dropbox.

Study on the tensile and wear properties of laser-cladded IN718 superalloy reinforced by carbon nanoproducts transformed from carbon nanotubes
Available formats
×

Send article to Google Drive

To send this article to your Google Drive account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Google Drive.

Study on the tensile and wear properties of laser-cladded IN718 superalloy reinforced by carbon nanoproducts transformed from carbon nanotubes
Available formats
×
×

Reply to: Submit a response

Please enter your response.

Your details

Please enter a valid email address.

Conflicting interests

Do you have any conflicting interests? *