Summary

For some multilayer systems that experience compression, buckling of the film in an initially debonded region may release energy that becomes available to drive the interface crack and increase the size of the debonded region. This phenomenon, called buckling delamination, occurs in structural composites where a compressed surface layer has debonded from its adjacent layers and buckles when the applied compression is sufficiently large. This surface layer may then delaminate if the interface toughness is not large enough to keep the interface crack from propagating. Buckling delamination is one of the most widely observed failure mechanisms in thin films and coatings on substrates when the stress is compressive. Buckling delamination involves the simultaneous interaction of buckling and interface cracking.

Two of the most commonly observed morphologies of buckling delaminations are seen in Figure 10.1. Both straight-sided and telephone cord delaminations have occurred in Figure 10.1(a) for a multilayered thin film deposited on a glass substrate where the film is subject to equi-biaxial compression. Straight-sided delaminations are rare under equi-biaxial compression. However, they are commonly observed when there is a dominant direction of compression in the film, in which case they propagate perpendicular to the direction of maximum compression. The telephone cord morphology is the mostly commonly observed morphology when the film is under equi-biaxial compression.

The buckle delamination in Figure 10.1(b) has formed under artificially constrained conditions created by patterning on the interface in a long narrowing wedge-shaped region of low adhesion before the film is deposited. The delamination, which takes place only within the low adhesion region, was initiated at the wide end and propagated towards the narrow edge, transitioning from the telephone cord morphology to the straight-sided morphology. Even when the film-substrate interface is not patterned, the delamination arrests along its sides and propagates at the curved front. Figure 10.2 shows a sequence of three closely spaced stages of the front propagation; the upper figures are a numerical solution discussed later, and the lower figures are the experimental observation.

This chapter develops the underlying mechanics of the buckling delamination with particular emphasis on the role of mixed-mode interface toughness, which is essential to understanding the existence, propagation and morphology of the various delamination modes.

Type
Chapter
Information
Publisher: Cambridge University Press
Print publication year: 2017

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Save book to Kindle

To save this book to your Kindle, first ensure coreplatform@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Buckling Delamination
  • Matthew R. Begley, University of California, Santa Barbara, John W. Hutchinson, Harvard University, Massachusetts
  • Book: The Mechanics and Reliability of Films, Multilayers and Coatings
  • Online publication: 13 July 2017
  • Chapter DOI: https://doi.org/10.1017/9781316443606.010
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Buckling Delamination
  • Matthew R. Begley, University of California, Santa Barbara, John W. Hutchinson, Harvard University, Massachusetts
  • Book: The Mechanics and Reliability of Films, Multilayers and Coatings
  • Online publication: 13 July 2017
  • Chapter DOI: https://doi.org/10.1017/9781316443606.010
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Buckling Delamination
  • Matthew R. Begley, University of California, Santa Barbara, John W. Hutchinson, Harvard University, Massachusetts
  • Book: The Mechanics and Reliability of Films, Multilayers and Coatings
  • Online publication: 13 July 2017
  • Chapter DOI: https://doi.org/10.1017/9781316443606.010
Available formats
×