Thermodynamic calculations have shown that chlorine can accumulate and cycle in the shaft of the blast furnace in the form of alkalis chlorides. Cycling of chlorine and alkalis in the upper part of the shaft was simulated at laboratory scale with a countercurrent reduction furnace (BORIS furnace) and also directly investigated at an industrial blast furnace. Experiments and calculations have shown the superposition of two cycles: one “pure” alkalis cycle in a large temperature domain, and a KCl cycle in a narrower range (600-1,000°C). According to the trials, effects of KCl on reduction and disintegration behaviour of sinter are similar to those of “pure” alkalis.

Type
Research Article
Copyright
© La Revue de Métallurgie, 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)