Improvement in High Temperature Oxidation Resistance of Co-Al-W Based Superalloys

  • Takahiko Ito (a1), Shogo Ikeda (a1) and Katsushi Tanaka (a1)

Abstract

Oxidation tests of Cr containing Co-based superalloys with compositions of Co-20at.%Ni-9at.%Al-9at.%W-x at.%Cr (x = 2, 4, 6, 8 and 10) have been carried out at 1173 and 1273 K in air. Oxidation resistance is improved upon alloying with Cr not only at 1173 K but also at 1273 K. The weight gain of the 10at.%Cr alloy oxidized at 1173 K is similar to that of the 5th generation Ni-based superalloy of TMS-173. Alloying with Cr is efficient to improve oxidation resistance, however, the shape of γ’ precipitates is rounded and the alignment of the precipitates along the <100> direction becomes less pronounced upon alloying with Cr.

Copyright

References

Hide All
1. Sato, J., Omori, T., Oikawa, K., Ohnuma, I., Kainuma, R., Ishida, K., Science 312, 90 (2006) .
2. Miura, S., Ohkubo, K. and Mohri, T., Mater. Trans. 48, 2403 (2007).
3. Suzuki, A., DeNolf, G.C., and Pollock, T.M., Scripta Mater. 56, 385 (2007).
4. Tanaka, K., Ohashi, T., Kishida, K. and Inui, H., Appl. Phys. Lett. 91, 181907 (2007).
5. Shinagawa, K., Omori, T., Sato, J., Oikawa, K., Ohnuma, I., Kainuma, R. and Ishida, K., Mater. Trans. 49, 1474 (2008).
6. Suzuki, A. and Pollock, T.M., Acta Mater. 56, 1288 (2008).
7. Osaki, M., Ueta, S., Shimizu, T., Omori, T. and Ishida, K., Denkiseikou 79, 197 (2008).
8. Chinen, H., Omori, T., Oikawa, K., Ohnuma, I., Kainuma, R. and Ishida, K., J. Phase Equi. Diffusion 30, 587 (2009).
9. Kobayashi, S., Tsukamoto, Y., Takasugi, T., Chinen, H., Omori, T., Ishida, K. and Zaefferer, S., Intermetallics 17, 1085 (2009).
10. Shinagawa, K., Omori, T., Oikawa, K., Kainuma, R. and Ishida, K., Scripta Mater. 61, 612 (2009).
11. Pollock, T.M., Dibbern, J., Tsunekane, M., Zhu, J. and Suzuki, A., JOM 62, 58 (2010).
12. Chen, M. and Wang, C.Y., Physics Letters A 374, 3238 (2010).
13. Bauer, A., Neumeier, S., Pyczak, F. and Goken, M., Scripta Mater. 63, 1197 (2010).
14. Ooshima, M., Tanaka, K., Okamoto, N.L., Kishida, K. and Inui, H., J. Alloys Comp. 508, 71 (2010).
15. Inui, H., Oohashi, T., Okamoto, N.L., Kishida, K. and Tanaka, K., Mater. Sci. Forum 638-642, 1342 (2010).
16. Okamoto, N.L., Oohashi, T., Adachi, H., Kishida, K., Inui, H. and Veyssiere, P., Phil. Mag. 91, 3667 (2011).
17. Klein, L., Bauer, A., Neumeier, S., Goken, M. and Virtanen, S., Corrosion Science 53, 2027 (2011).
18. Klein, L., Shen, Y., Killian, M.S. and Virtanen, S., Corrosion Science 53, 2713 (2011).
19. Kobayashi, S., Tsukamoto, Y. and Takasugi, T., Intermetallics 19, 1908 (2011).
20. Tanaka, K., Ooshima, M., Tsuno, N., Sato, A. and Inui, H., Phil. Mag. 92, 4011 (2012).
21. Titus, M.S., Suzuki, A., Pollock, T.M., Scripta Mater. 66, 574 (2012).
22. Bauer, A., Neumeier, S., Pyczak, F., Singer, R.F. and Goken, M., Mater. Sci. Eng. A 550, 333 (2012).
23. Meher, S., Yan, H.Y., Nag, S., Dye, D. and Banerjee, R., Scripta Mater. 67, 850 (2012).
24. Omori, T., Oikawa, K., Sato, J., Ohnuma, I., Kattner, U.R., Kainuma, R. and Ishida, K., Intermetallics 32, 274 (2013).
25. Klein, L., Killian, M.S. and Virtanen, S., Corrosion Science 69, 43 (2013).
26. Vermaak, N., Mottura, A. and Pollock, T.M., Corrosion Science 75, 300 (2013).
27. Zaplatynsky, I., Oxid. Metals, 11, 289 (1977).

Keywords

Metrics

Full text views

Total number of HTML views: 0
Total number of PDF views: 0 *
Loading metrics...

Abstract views

Total abstract views: 0 *
Loading metrics...

* Views captured on Cambridge Core between <date>. This data will be updated every 24 hours.

Usage data cannot currently be displayed