Hostname: page-component-76fb5796d-r6qrq Total loading time: 0 Render date: 2024-04-26T09:41:20.501Z Has data issue: false hasContentIssue false

High Reliability Underfill for Flip-Chip Application

Published online by Cambridge University Press:  10 February 2011

K. Sumita
Affiliation:
Silicone Electronic Material Research Center, Shin‐Etsu Chemical Co., 1‐10 Hitomi Matsuida, Gunma, 379‐02 Japan
K. Kumagae
Affiliation:
Silicone Electronic Material Research Center, Shin‐Etsu Chemical Co., 1‐10 Hitomi Matsuida, Gunma, 379‐02 Japan
K. Dobashi
Affiliation:
Silicone Electronic Material Research Center, Shin‐Etsu Chemical Co., 1‐10 Hitomi Matsuida, Gunma, 379‐02 Japan
T. Shiobara
Affiliation:
Silicone Electronic Material Research Center, Shin‐Etsu Chemical Co., 1‐10 Hitomi Matsuida, Gunma, 379‐02 Japan
M. Kuroda
Affiliation:
Japan Package Technology Development, Intel Japan K.K., 5‐6 Tokoudai Tsukuba, Ibaraki, 300‐26 Japan,
Get access

Abstract

A new underfill was developed for a flip chip application with a large VLSI die. The new underfill is resistant to hydrolysis, exhibits a significantly lower moisture saturation level than widely used carboxylic anhydride cured underfills, demonstrates superb penetration capability between such a large die and an organic substrate without void formation, and delivers excellent adhesion characteristics and reliability performance during temperature cycling test and PCT (pressure cooker test).

The new underfill utilizes amine catalyzed ring opening polymerization of epoxides, forms ether linkages during cure rather than ester linkages which anhydride cured underfills form, and strongly resists to hydrolysis. The underfill is less sensitive to moisture contamination and provides improved floor life as well as storage life in contrast to anhydride cured underfills as well. Unique low stress performance and penetration capability of the underfill are attributed to the use of proprietary silicone modified epoxy resin as well as highly loaded filler of optimized size, shape and size distribution in reference to the gap between a die and an organic substrate.

An optimum cure schedule and a desirable viscosity range have also been identified for the new underfill to minimize filler segregation. Proper preheating of a die‐substrate has effectively reduced void formation while facilitating the removal of volatile from an organic substrate.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Koopman, N. G., Reiley, T. C. and Tolta, P. A., “High density chip interconnections”, ISHM '88 Proc, pp.295300 (1988)Google Scholar
2 Suryanarayana, D., Hsiao, R., Gall, T.P., McCreary, J.M., “Enhancement of Flip‐Chip Fatigue Life by Encapsulation”, IEEE, pp 218223, vol 14, No 1., Mar., 1991 Google Scholar
3 Suryanarayana, D., Wu, T. Y. and Varcoe, J. A., “Encapsulants Used in Flip Chip Packages”, Proceedings of the 43rd Electronic Components & Technology Conference, 1993, pp. 193198 Google Scholar
4 Niibo, M.,Hand Book of Epoxy resin, Nikkan Industrial Newspaper Co., pp.206209 Google Scholar
5 Soga, T., Nakano, F. and Fuyama, M., “Development of a high‐reliability flip‐chip packaging reinforced by resin”, ELECTRONICS and COMMUNICATIONS in JAPAN, 71, pp. 1927 (Nov., 1988)Google Scholar
6 Rai, A., Dotta, Y., Nukii, T., Ohnish, T., “Flip‐Chip COB Technology on PWB”, IMC, 1992 Proceedings, pp. 144149, Jun.(1992)Google Scholar
7 Niibo, M..Hand Book of Epoxy resin, Nikkan Industrial Newspaper Co., pp.203205 Google Scholar