Chemical Stability of Simiulated HLW Forms in Contact With Clay Media+

Published online by Cambridge University Press:  15 February 2011

P. Van Iseghem
Affiliation:
Materials Science Department, S.C.K./C.E.N., B-2400 MOL (Belgium);
W. Timmerans
Affiliation:
Materials Science Department, S.C.K./C.E.N., B-2400 MOL (Belgium);
R. De Batist
Affiliation:
Also Rijksuniversitair Centrum, Antwerpen, B-2020 ANIWERPEN (Belgium).
Get access

Abstract

The corrosion stability of six simulated HLW forms proposed by several European countries (five borosilicate glasses and one borosilicate glass ceramic) in contact with different media relating to the clay disposal has been investigated for periods up to 80 days and at a surface area to solution volume ratio of 1 cm−1 under non de-aerated conditions. In the reference medium distilled water the corrosion stabilities are largely determined by saturation effects for elements such as Si, Ca, Mg, Sr, Fe and U. Si saturation is found to be enhanced by a large Al2O3 concentration in the glass. In the clay-water mixture these saturation effects are much less predominant. Wet clay attacks the waste forms faster than the clay-water mixture, although the corrosion rates tend to decrease with time in both clay media. In general, no simple Arrhenius-type temnnerature dependence for the corrosion behaviour is found for the interval between 40 and 200°C.

Type
Research Article
Copyright
Copyright © Materials Research Society 1982

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Footnotes

+

Supported in part by the Camnission of the European Communities

References

REFERENCES

1. Marples, J.A.C. et al. “Testing and evaluation of the properties of vaxious potential materials for immobilising high activity waste”, EUR 7138 EN (1981).Google Scholar
2. Van Iseghem, P. et al. “Interaction of vitrified high level waste with clay environment”, Proc. International Seminar on Chemistry and Process Engineeringfor High-Level Liquid Waste Solidification, Jülich (F.R. Germany), June 1981, in press.Google Scholar
3. Clark, D.E. et al. “Corrosion of glass”, Books for Industry (New York), 1979 Google Scholar
4. Hench, L.L. et al. “Physical Chemistry of glass surfaces”, J. non Cryst. Sol. 28 (1978), 83105 Google Scholar
5. Iler, R.K. “Effect of adsorbed alumina on the solubility of amorphous silica in water”, J. of Coll. and Interf. Science, 43 (1973), no 2, 399408.Google Scholar
6. Fullam, H.T. “Solubility effects in waste-glass/demineralized-water systems”, PNL 3614 (1981).Google Scholar
7. Barkatt, A. et al. “Evaluation of chemical stability of vitrification media for radioactive waste products”, Phys. and Chem. of Glasses, 22 (1981) no 4, 7385.Google Scholar
8. Lokken, R.O. “Leaching behaviour of glass ceramic nuclear waste forms”, PWL 4022 (1981).CrossRefGoogle Scholar
9. Garrels, R.M. et al. “Solutions, minerals and equilibria”, Harper and Row, (New York), 1965.Google Scholar
10. Lanza, F. et al. “Methodology of leach testing of borosilicate glasses in water”, Proc. First European Community Conference on Radioactive Waste Management and Disposal, Luxembourg (1980).Google Scholar