Abstract

Ti-47at%Al+7vol%(TiN+TiB2) alloys, produced by the Martin Marietta XD process, were subjected to tensile constant stress creep deformation in the range 760-850°C temperature and 138–276 MPa (20–40 ksi) stress. These alloys have a matrix of TiAl and Ti3Al initially containing 1 to 10 μm diameter equiaxed particles of Ti2B and Ti2AlN. Microstructures were examined using optical, SEM and TEM methods in an attempt to correlate the substructures with the property data. In particular, fine coherent particles have been observed to decorate dislocations and the interior of TiAl grains. The presence of these particles is thought to explain the creep resistance of this alloy.

Type
Research Article
Copyright
Copyright © Materials Research Society 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Lipsitt, H.A. in High Temperature Ordered Intermetallic Alloys, edited by Koch, C.C., Liu, C.T. and Stoloff, N.S. (Mater. Res. Soc. Proc. 39, Pittsburgh, PA 1985) pp.351364.Google Scholar
2. Kim, J.W., J. of Metals, 41, 24 (1989).Google Scholar
3. Mendiratta, M.G. and Lipsitt, H.A., J. Mat Sci., 15, 2985 (1980).Google Scholar
4. Martin, P.L., Mendiratta, M.G., Lipsitt, H.A., Metall. Trans., 14A, 2170 (1983).Google Scholar
5. Martin, P.L. and Lipsitt, H.A., “Deformation and Fracture of TiAl + W at Elevated Temperatures,” edited by Wilshire, B. and Evans, R.W., (Proc. International Conf. on Creep and Fracture of Eng. Materials and Structures, 4, Inst. of Metals, London, 1990) p. 255.Google Scholar
6. Takahashi, T., Nagai, H. and Oikawa, H., J.Japan Inst. Metals, 53, 471 (1989).Google Scholar
7. Loiseau, A. and Lasalmonie, A., Materials Sci. and Eng., 67, 163 (1984).Google Scholar
8. Loiseau, A. and Lasalmonie, A., Acta Cryst., B39, 580 (1983).Google Scholar
9. Kaufman, M.J., Konitzer, D.G., Shull, R.D. and Fraser, H.L., Scripta Metal., 20, 103 (1986).Google Scholar
10. Lipsitt, H.A., Shechtman, D., and Schafrik, R.E., Metall. Trans., 6A, 1991 (1975).Google Scholar
11. Evans, R.W. and Wilshire, B., Creep of Metals and Alloys, (Institute of Metals, London, 1985).Google Scholar
12. Hirsch, P., Howie, A., Nicholson, R.B., Pashley, D.W. and Whelan, M.J., Electron Microscopy of Thin Crystals, (Krieger Publishing, Huntington, NY, 1977), p. 327.Google Scholar
13. Villars, P. and Calvert, L.D., Pearson's Handbook of Crystallographic Data for Intermetallic Compounds, (ASM, Metals Park, OH, 1985).Google Scholar
14. Cozar, R. and Pineau, A., Metail. Trans., 4, 47 (1973).Google Scholar