Atom Probe Tomographic Investigation of the Solute Segregation to Crystal Defects in γ-phase Co-35Ni-20Cr-10Mo Superalloy
Published online by Cambridge University Press: 30 July 2020
Abstract
An abstract is not available for this content so a preview has been provided. As you have access to this content, a full PDF is available via the ‘Save PDF’ action button.
![Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'](https://static.cambridge.org/content/id/urn%3Acambridge.org%3Aid%3Aarticle%3AS1431927620023740/resource/name/firstPage-S1431927620023740a.jpg)
- Type
- Collaborative Analysis Using Atom Probe Tomography Including TEM/APT Characterization of Metal Alloys and Other Material Systems
- Information
- Copyright
- Copyright © Microscopy Society of America 2020
References
Singh, R.P. and Doherty, R.D., Metallurgical Transactions 23A (1992), p. 307.10.1007/BF02660873CrossRefGoogle Scholar
Sorensen, D. et al. ., Acta Materialia 63 (2014), p. 63.10.1016/j.actamat.2013.10.005CrossRefGoogle Scholar
Smith, T.M. et al. ., Nature Communications 7 (2016), p. 13434.10.1038/ncomms13434CrossRefGoogle Scholar
Palanisamy, D. et al. ., Scripta Materialia 155 (2018), p. 144.10.1016/j.scriptamat.2018.06.037CrossRefGoogle Scholar
Barba, D. et al. ., Scripta Materialia 127 (2017), p. 37.10.1016/j.scriptamat.2016.08.029CrossRefGoogle Scholar
SA would like to acknowledge financial support from the Alexander von Humboldt Foundation.Google Scholar