SiC–Al–Si composites by rapid pressureless infiltration in air

Published online by Cambridge University Press:  03 March 2011

X.F. Yang
Affiliation:
Materials Research and Education Center, 201 Ross Hall, Auburn, University, Auburn, Alabama 36849
X.M. Xi
Affiliation:
Materials Research and Education Center, 201 Ross Hall, Auburn, University, Auburn, Alabama 36849
Get access

Abstract

A rapid, pressureless infiltration technique for fabricating SiC-reinforced Al-Si composites is described. The infiltration can be performed by simply dipping a ceramic preform into a molten alloy in an open air environment. This method makes it possible to produce composites that contain a high volume fraction (80%) of a variety of ceramic reinforcements, including particulates and fibers. This technique has potential for low-cost and versatile production of SiC-Al-Si composites for many industrial applications, such as automobile components and electronic packaging.

Type
Rapid Communication
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Zweben, C., JOM 44(7), 15 (1992).CrossRefGoogle Scholar
2Premkumar, M. K., Hunt, W. H. Jr., and Sawtell, R.R., JOM 44(7), 24 (1992).CrossRefGoogle Scholar
3Allison, J. E. and Cole, G. S., JOM 45(1), 19 (1993).CrossRefGoogle Scholar
4Mortensen, A. and Koczak, M. J., JOM 45(3), 10 (1993).CrossRefGoogle Scholar
5Lai, S. W. and Chung, D.D.L., J. Mater. Sci. 29, 3128 (1994).CrossRefGoogle Scholar
6Clyne, T. W. and Withers, P. J., An Introduction to Metal Matrix Composites (Cambridge University Press, 1993).CrossRefGoogle Scholar
7White, D. R., Urquhart, A. W., Aghajanian, M. K., and Creber, D.K., U.S. patent 4,828,008; May 9, 1989.Google Scholar
8Lin, R. Y., Warrier, S. G., Blue, C. A., Chen, C. C., Eppich, C. A., and Blue, R.A., JOM 46(3), 26 (1994).CrossRefGoogle Scholar
9Messner, R. P. and Chiang, Y. M., J. Am. Ceram. Soc. 73, 1193 (1990).CrossRefGoogle Scholar
10Ness, J. N. and Page, T. F., J. Mater. Sci. 21, 1377 (1986).CrossRefGoogle Scholar
11Singh, M. and Behrendt, D. R., NASA Technical Memorundum 105860 (1992).Google Scholar
12Hillig, W. B., Am. Ceram. Soc. Bull. 73(4), 56 (1994).Google Scholar
13Skibo, M. D. and Schuster, D. M., U.S. patent 4,759,995; July 26, (1988).Google Scholar
14Viala, J. C., Fortier, P., and Bouix, J., J. Mater. Sci. 25, 1842 (1990).CrossRefGoogle Scholar