Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Ikezawa, Kazuhiro
and
Maruyama, Tadashi
2002.
Sharp tip geometry and its effect on hardness in nanoindentation experiments.
Journal of Applied Physics,
Vol. 91,
Issue. 12,
p.
9689.
Kouitat-Njiwa, R
and
von Stebut, Jürgen
2003.
Boundary element numerical analysis of elastic indentation of a sphere into a bi-layer material.
International Journal of Mechanical Sciences,
Vol. 45,
Issue. 2,
p.
317.
Ma, Shengli
Ma, Dayan
Xu, Kewei
and
Jie, Wanqi
2004.
Structural characterization of nanocomposite Ti–Si–N coatings prepared by pulsed dc plasma-enhanced chemical vapor deposition.
Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena,
Vol. 22,
Issue. 4,
p.
1694.
Suganuma, Motohiro
and
Swain, Michael V.
2004.
Simple method and critical comparison of frame compliance and indenter area function for nanoindentation.
Journal of Materials Research,
Vol. 19,
Issue. 12,
p.
3490.
Tang, Wu
Shen, Lu
and
Xu, Kewei
2005.
Hardness and elastic modulus of Au/NiCr/Ta multilayers on Al2O3 substrate by nanoindentation continuous stiffness measurement technique.
Thin Solid Films,
Vol. 485,
Issue. 1-2,
p.
72.
Tan, Mengxi
2006.
A study of indentation work in homogeneous materials.
Journal of Materials Research,
Vol. 21,
Issue. 6,
p.
1363.
Wang, Tao
de las Heras Alarcón, Carolina
Goikoetxea, Monika
Beristain, Itxaso
Paulis, Maria
Barandiaran, Maria J.
Asua, José M.
and
Keddie, Joseph L.
2010.
Cross-Linked Network Development in Compatibilized Alkyd/Acrylic Hybrid Latex Films for the Creation of Hard Coatings.
Langmuir,
Vol. 26,
Issue. 17,
p.
14323.
Kailasanathan, C.
and
Selvakumar, N.
2012.
Comparative study of hydroxyapatite/gelatin composites reinforced with bio-inert ceramic particles.
Ceramics International,
Vol. 38,
Issue. 5,
p.
3569.
N, Selvakumar
and
R, Malkiya Rasalin Prince
2017.
Microstructure, surface topography and sliding wear behaviour of titanium based coating on AISI 1040 steel by magnetron sputtering.
Archives of Civil and Mechanical Engineering,
Vol. 17,
Issue. 2,
p.
281.
Selvakumar, N.
and
Malkiya Rasalin Prince, R.
2018.
Adhesion Behaviour, Nanohardness and Surface Roughness of Ti–6Al–4V–6B4C Thin Films Grown on AISI 1040 Steel.
Transactions of the Indian Institute of Metals,
Vol. 71,
Issue. 4,
p.
893.
Chen, Juan
Shi, Junqin
Wang, Yunpeng
Sun, Jiapeng
Han, Jing
Sun, Kun
and
Fang, Liang
2018.
Nanoindentation and deformation behaviors of silicon covered with amorphous SiO2: a molecular dynamic study.
RSC Advances,
Vol. 8,
Issue. 23,
p.
12597.
Chen, Juan
Shi, Junqin
Chen, Zhi
Zhang, Meng
Peng, Weixiang
Fang, Liang
Sun, Kun
and
Han, Jing
2019.
Mechanical properties and deformation behaviors of surface-modified silicon: a molecular dynamics study.
Journal of Materials Science,
Vol. 54,
Issue. 4,
p.
3096.
Jha, Rajesh
and
Agarwal, Arvind
2021.
Software (GUI/APP) for Developing AI-Based Models Capable of Predicting Load-Displacement Curve and AFM Image during Nanoindentation.
Coatings,
Vol. 11,
Issue. 3,
p.
299.