Effects of microstructure constituents of α2-Ti3Al/γ-TiAl lamellae, β-Ti grains and γ grains, with various volume fractions on room-temperature ductility of γ-TiAl based alloys have been studied. The ductility of the alloys containing β phase of about 20% in volume increases to more than 1% as the volume fraction of γ phase increases to 80%. However, γ single phase alloys show very limited ductility of less than 0.2%. The present results, thus, confirmed the significant contribution of β phase to enhancement of the room-temperature ductility in multi-component TiAl alloys.