We have demonstrated a uniform, robust interface for high-k deposition with significant improvements in device electrical performance compared to conventional surface preparation techniques. The interface was a thin thermal oxide that was grown and then etched back in a controlled manner to the desired thickness. Utilizing this approach, an equivalent oxide thickness (EOT) as low as 0.87 nm has been demonstrated on high-k gate stacks having improved electrical characteristics as compared to more conventionally prepared starting surfaces.