Hostname: page-component-848d4c4894-r5zm4 Total loading time: 0 Render date: 2024-07-01T19:00:32.857Z Has data issue: false hasContentIssue false

Study of simulated HLW-glass leaching behavior under low oxygen repository condition

Published online by Cambridge University Press:  21 March 2011

Zhang Hua*
Affiliation:
Radiochemistry Department, China Institute of Atomic Energy, P.O.Box 275(93), Beijing, 102413, P.R.China
Luo Shanggeng
Affiliation:
Radiochemistry Department, China Institute of Atomic Energy, P.O.Box 275(93), Beijing, 102413, P.R.China
*
Corresponding author: Tel: +86-010-69357445; Fax: +86-010-69358509 E-mail: nzhangh@yahoo.com.cn
Get access

Abstract

Many countries have recognized vitrification as the suitable solidification method for conditioning high level radioactive waste before they are isolated from biosphere in geologic disposal. This paper studies the leaching behavior of a simulated HLW-glass (90Nd/10) under low oxygen repository condition during 1.5 years. The leaching results showed that the glass was corroded less under low oxygen condition than under ambient atmosphere. XRD analyses showed some little diffraction peak appeared on the leached glass surface at 150°C. At the same time, no diffraction peak appeared on the leached glass surface at 90°C. The secondary products formed on the surface of the leached glass contained mainly Si, Al, Ca and Fe.

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] An international group of experts, the management of radioactive waste, Published by the uranium institute. USA. (1991).Google Scholar
[2] International Atomic Energy Agency, Design and Operation of High Level Waste Vitrification and Storage Facilities. IAEA Technical Reports Series No.339. (1992)Google Scholar
[3] MCC, MCC-1P static leaching test method, Nuclear Waste Materials Handbook Test Methods, Material Characterization Center, U.S.A. (1983)Google Scholar
[4] Hua, Zhang, Jianwen, Yang, Baojun, Li, Shanggeng, Luo, Stability of HLW glass under simulated repository conditions, The Third Korea-China Joint Workshop on Nuclear Waste Management, Shanghai, China. July.8-10. (2002)Google Scholar
[5] Standard Test Method for Static Leaching of Monolithic Waste Forms for Disposal of Radioactive Waste, ASTM Designation: C 1220-98, (1999)Google Scholar
[6] Shurong, Xu, Properties Evaluation and Establishment of Mathematical Models on Simulated High-level waste Glass Forms Melted in the First Cold–bench Scale Test,, the master paper of China Institute of Atomic Energy. (2001)Google Scholar
[7] Harvey, K.B., Dissolution Models for Glassy Waste Forms, Atomic Energy of Canada Limited, Whiteshell laboratories, Pinawa, Manitoba ROE ILO. (1995)Google Scholar
[8] Chengyu, Wang, Yin, Tao, Glass surface and surface treatment, Beijing, published by China constructing material industry, Nov. (1993)Google Scholar