Role of Annealing for Improving Hydrogen Storage Properties of Ti-Cr-V Alloy

Published online by Cambridge University Press:  26 February 2011

Yasuhiro Munekata
Affiliation:
y-mune@eng.hokudai.ac.jp, Hokkaido University, Graduate School of Engineering, N-13, W-8, Kita-ku, Sapporo, 0608628, Japan
Kota Washio
Affiliation:
washio@eng.hokudai.ac.jp, Hokkaido University, Graduate School of Engineering, Sapporo, N/A, Japan
Takanori Suda
Affiliation:
suda@eng.hokudai.ac.jp, Hokkaido University, Graduate School of Engineering, Sapporo, N/A, Japan
Naoyuki Hashimoto
Affiliation:
hasimoto@eng.hokudai.ac.jp, Hokkaido University, Graduate School of Engineering, Sapporo, N/A, Japan
Somei Ohnuki
Affiliation:
ohnuki@eng.hokudai.ac.jp, Hokkaido University, Graduate School of Engineering, Sapporo, N/A, Japan
Hironobu Arashima
Affiliation:
hironobu_arashima@jsw.co.jp, Japan Steel Works, Muroran Res. Inst., Muroran, N/A, Japan
Hideaki Ito
Affiliation:
hideaki_ito@jsw.co.jp, Japan Steel Works, Muroran Res. Inst., Muroran, N/A, Japan
Get access

Abstract

One of impotent materials issues of Ti-Cr-V based hydrogen storage alloys is to improve cyclic degradation of storage capacity, which has been assumed to be the effect of internal stress. We focused on the sub-micron structure of this material, which can be accumulated during cyclic use. We used 24Ti-36Cr-40V alloy for the specimens, after FZ melting. Powered samples were fabricated by mechanical grinding under Ar environment. Vacuum annealing was carried out for reducing residual stress and lattice defects. PCT properties were tested at 293 K under 4.5 MPa. XRD and TEM were carried out for important samples. In the first cycle, the annealing resulted in the increasing of storage capacity, but in the second cycle the improving was disappeared. Comparing microstructures with and without annealing, complex dislocation structures were observed after cyclic hydrogenation. It is notable that dislocation free structure was some time observed in the fine grains of less than 0.1 micron, which suggests the possibility of fine structure without defect accumulation.

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Inui, H., Yamamoto, T., Hirota, M. and Yamaguchi, M., J. Alloys Comp. 330–332, 117124, (2002)Google Scholar
[2] Yokoyama, T., Metal, 73, 463468, (2003)Google Scholar
[3] Uchida, H., Int. J. Hydrogen Energy, 24, 861869, (1999)Google Scholar
[4] Ho, H. and Lee, J., J. Alloy Comp. 202, 2328, (1993)Google Scholar
[5] Itoh, H., Arashima, H., Kubo, K., Kabutomori, T. and Ohnishi, K., J. Alloy. Comp. 404–406, 417420, (2005)Google Scholar
[6] Takase, K., Master thesis, Hokkaido University, (2005)Google Scholar
[7] Itoh, H., Arashima, H., Kubo, K. and Kabutomori, T., J. Alloys Comp. 330–332, 287291, (2002)Google Scholar
[8] Arashima, H., Takahashi, F., Ebisawa, T., Itoh, H. and Kabutopmori, T., Alloys Comp. 356–357, 405408, (2003)Google Scholar
[9] Itoh, H., Arashima, H., Kubo, K., Kabutomori, T. and Ohnunishi, K., J. Alloys Comp. 404–406, 417420, (2005)Google Scholar
[10] ohnuki, S., Takase, K., Yashiki, K., Hamada, K., Suda, T. and Watanabe, S.: Korean Soc. Elec. Micro, 36, 5761, (2006)Google Scholar
[11] Hall, W. H., J. Inst. Metals, 75, 1127, (1950)Google Scholar