Plasma Etching of InP and Related Materials in Electron Cyclotron Resonance CH4/H2/Ar Discharges

Published online by Cambridge University Press:  21 February 2011

S. J. Pearton
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ
U. K. Chakrabarti
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ
A. P. Kinsella
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ
A. B. Emerson
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ
D. Johnson
Affiliation:
Plasma Therm, Inc., Voorhees, NJ
C. Constantine
Affiliation:
Plasma Therm, Inc., Voorhees, NJ
Get access

Abstract

We have investigated the etch rates, residual lattice damage, surface morphologies and chemistries of InP, InGaAs, AlInAs and GaAs plasma etched in electron cyclotron resonance (ECR) CH4/H2/Ar discharges. The etch rates of InP and InGaAs increase linearly with additional RF biasing of the substrate, and are approximately a factor of two faster than for GaAs. Under our conditions the etch rate of Al0.52Ga0.48As is very low (˜25 Å - min−1) even for the addition of 100 V RF bias. In all of these materials the residual damage layer remaining after dry etching is very shallow (˜20 Å) as evidenced from Schottky barrier height and photoluminescence measurements combined with wet chemical etching. InP shows significant P depletion with the addition of RF biasing during the ECR etching while GaAs retains a near-stoichiometric surface. Hydrogen passivation of shallow donors in n-type GaAs occurs to a depth of ˜3000,Å during exposure to the CH4/H2/Ar discharge for long periods (60 mins). The surface morphologies of the In-based materials become roughened for etching with the addition of RF biasing while GaAs displays smooth, residue-free surfaces under these conditions.

Type
Research Article
Copyright
Copyright © Materials Research Society 1991

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] See for example “Dry Etching for Microelectronics,” ed. Powell, R. A., Vol 4 of Materials Processing Theory and Practices (North Holland, Amsterdam 1984).Google Scholar
[2] Pang, S. W., Goodhue, W. D., Lyszczarz, T. M., Ehrlich, D. J., Goodman, R. B. and Johnson, G. D., J. Vac. Sci, Technol. B6 1916 (1988).Google Scholar
[3] See the discussion in Skidmore, K., Semiconductor International, pp. 74–79, June 1979.Google Scholar
[4] Asmussen, J., J. Vac. Sci. Technol. A7 883 (1989).Google Scholar
[5] Cheung, R., Lee, Y. H., Lee, K. Y., Smith, T. P. III, Kera, D. P., Beaumont, S. D. and Wilkinson, C. D., J. Vac. Sci. Technol. B7 1462 (1989).Google Scholar
[6] Hayes, T. R., Dreisbach, M. A., Thomas, P. M., Dautremont-Smith, W. C. and Heimbrook, L. A., J. Vac. Sci. Technol. B7 1130 (1989).Google Scholar
[7] Schmid, H. in Proc. 6th Intl. Conf. on Ion and Plasma Assisted Techniques, Brighton UK (Elselvier, NY 1987) p. 98.Google Scholar
[8] Pearson, S. J., Chakrabarti, U. K. and Baiocchi, F. A., Appl. Phys. Lett. 55 1633 (1989).Google Scholar
[9] Hayes, T. R., Chakrabarti, U. K., Baiocchi, F. A., Emerson, A. B., Luftman, H. S. and Dautremont-Smith, W. C. (unpublished).Google Scholar