Novel N2O Plasma Passivation on Polycrystalline Silicon Thin-Film Transistors

Published online by Cambridge University Press:  10 February 2011

Fang-Shing Wang
Affiliation:
Department of Electronics Engineering and Institute of Electronics, Semiconductor Research Center, National Chiao Tung University, National Nano Device Laboratory, Hsinchu, Taiwan, R.O.C
Chun-Yao Huang
Affiliation:
Department of Electronics Engineering and Institute of Electronics, Semiconductor Research Center, National Chiao Tung University, National Nano Device Laboratory, Hsinchu, Taiwan, R.O.C
Huang-Chung Cheng
Affiliation:
Department of Electronics Engineering and Institute of Electronics, Semiconductor Research Center, National Chiao Tung University, National Nano Device Laboratory, Hsinchu, Taiwan, R.O.C
Get access

Abstract

A novel defect passivation process of polycrystalline silicon thin-film transistors (poly-Si TFT's) utilizing nitrous oxide (N2O) plasma was investigated. In terms of the gas flow rate, chamber pressure, and plasma exposure time, the optimum plasma condition has been found to significantly improve the electrical characteristics of poly-Si TFTs. The performance is even better than those passivated with conventional hydrogen plasma. It is believed that the nitrogen radicals from the N2O gas as well as the hydrogen ones from the residual H2O both can diffuse into the gate-oxide/poly-Si interface and the channel poly-Si layer to passivate the defect-states. Furthermore, the gate-oxide leakage current significantly decreases and the oxide breakdown voltage slightly increases after applying N2O-plasma treatment. This novel process is promising for the applications of TFT/liquid crystal displays and TET/static random access memories.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Kamins, T. I. and Marcoux, P. J., IEEE Electron Device Lett., EDL–1, 159 (1980).Google Scholar
2. Migliorato, P., and Meakin, D. B., Applied Surface Sci., 30, 353 (1987).Google Scholar
3. Wu, I-W., Huang, T-Y., Jackson, W. B., Lewis, A. G., and Chiang, A. C., IEEE Electron Device Lett., EDL–12, 181 (1991).Google Scholar
4. Ikeda, S., Hashiba, S., Kuramoto, I., Katoh, H., Ariga, S., Yamanaka, T., Hashimoto, T., Hashimoto, N. and Meguro, S., IEDM Tech. Dig., 459 (1990).Google Scholar
5. Chern, H. N., Lee, C. L., and Lei, T. F., IEEE Trans. Electron Devices, ED–40, 2301 (1993).Google Scholar
6. Nickel, N. H., Yin, A. and Fonash, S. J., Appl. Phys. Lett., 65, 3099 (1994).Google Scholar
7. Tsai, M. J., Wang, F. S., Cheng, K. L., Wang, S. Y., Feng, M. S., and Cheng, H. C., Solid State Electronics, 38, 1233 (1995).Google Scholar
8. Wang, F. S., Tsai, M. J., and Cheng, H. C., IEEE Electron Device Lett., EDL–16, p.503.Google Scholar
9. Levinson, J., Shepherd, F. R., Scanlon, P. J., Westwood, W. D., Este, G., and Rider, M., J. AppI. Phys., 53, 1193 (1982).Google Scholar
10. Proano, R. E., Misage, R. S., and Ast, D. G., IEEE Trans. Electron Devices, ED–36, 1915 (1989).Google Scholar
11. Momose, H. S., Morimoto, T., Ozawa, Y., Yamabe, K., and Iwai, H., IEEE Trans. Electron Devices, ED–41, 546 (1994).Google Scholar