Hostname: page-component-77c89778f8-sh8wx Total loading time: 0 Render date: 2024-07-21T18:39:46.801Z Has data issue: false hasContentIssue false

Towards a more Realistic Experimental Protocol for the Study of Atmospheric Chloride-Induced Stress Corrosion Cracking in Intermediate Level Radioactive Waste Container Materials

Published online by Cambridge University Press:  03 July 2014

A.B. Cook
Affiliation:
Corrosion and Protection Centre, School of Materials, The University of Manchester, Oxford Road, Manchester M13 9PL, UK.
B. Gu
Affiliation:
Corrosion and Protection Centre, School of Materials, The University of Manchester, Oxford Road, Manchester M13 9PL, UK.
S.B. Lyon
Affiliation:
Corrosion and Protection Centre, School of Materials, The University of Manchester, Oxford Road, Manchester M13 9PL, UK.
R.C. Newman
Affiliation:
Department of Chemical Engineering and Applied Chemistry, University of Toronto, 200 College Street, Toronto, Ontario, M5S 3E5, Canada.
D.L. Engelberg
Affiliation:
Corrosion and Protection Centre, School of Materials, The University of Manchester, Oxford Road, Manchester M13 9PL, UK. Research Centre for Radwaste and Decommissioning, The University of Manchester, Oxford Road, Manchester M13 9PL, UK.
Get access

Abstract

The occurrence of Atmospheric chloride-Induced Stress Corrosion Cracking (AISCC) under wetted deposits of MgCl2 or sea-salt at 70°C has been investigated at various Relative Humidities (RH). The appearance of AISCC is a function of the environmental RH. At 33% RH (the deliquescence point of MgCl2), AISCC generated under MgCl2 or sea-salt deposits is of a similar appearance with regards to the number of cracks produced and average crack length. At 50% RH sea-salt seems to be more aggressive at least in terms of crack frequency. This observation may highlight the significance of carnallite (KMgCl3.6H2O) in promoting AISCC in types 304L and 316L stainless steels. The use of accelerated testing methods to validate apparent thresholds in chloride deposition density and other critical factors that influence the initiation and propagation of AISCC is briefly discussed.

Type
Articles
Copyright
Copyright © Materials Research Society 2014 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Shoji, S. and Ohnaka, N., Boshoku Gijutsu (Corrosion Engineering JP, English Edition), 38 (1989) 111.Google Scholar
Truman, J. and Pirt, K., Corros. Sci., 17 (1977) 71.CrossRefGoogle Scholar
Iversen, A. and Prosek, T., “Atmospheric stress corrosion cracking of austenitic stainless steels in conditions modeling swimming pool halls”, Eurocorr 2007, EFC, Freiburg im Breisgau, Germany, Paper No. 1142.Google Scholar
Prosek, T., Iversen, A. and Taxen, C., “Low Temperature Stress Corrosion Cracking of Stainless Steels in the Atmosphere in Presence of Chloride Deposits”, Corrosion 2008, New Orleans, LA, Paper No. 08484.Google Scholar
Cook, A., Duff, J., Stevens, N., Lyon, S., Sherry, A. and Marrow, T.J., ECS Transactions, 25 (2010) 119.10.1149/1.3407553CrossRefGoogle Scholar
Fairweather, N.D., Platts, N. and Tice, D.R., “Stress corrosion crack initiation in type 304 stainless steel in atmospheric environments containing chloride: Influence of surface condition, relative humidity, temperature and thermal sensitization”, Corrosion 2008, New Orleans, LA, Paper No. 08485.Google Scholar
Albores-Silva, O.E., Charles, E.A. and Padovani, C., CEST, 46 (2011) 124.10.1179/1743278210Y.0000000004CrossRefGoogle Scholar
ASTM International G 30 – 97, “Standard practice for making and using U-Bend stress-corrosion test specimens” (2009).Google Scholar
Greenspan, L., J. Res. NBS., 81A (1977) 89.CrossRefGoogle Scholar
King, F., Robinson, P., Watson, C., Burrow, J. and Padovani, C., “ACSIS – A model to Assess the Potential for Atmospheric Corrosion of Stainless Steel ILW Containers During Storage and the Operational Phase of a UK Geological Disposal Facility”, Corrosion 2013, Orlando, FL, Paper No. 02717.Google Scholar
Cook, A., unpublished results.Google Scholar
Lillard, R.S., Kolman, D.G., Hill, M.A., Prime, M.B., Veirs, D.K., Worl, L.A. and Zapp, P. (and references contained therein), Corrosion 65, (2009) 175.10.5006/1.3319126CrossRefGoogle Scholar
Cook, A. B., Stevens, N., Duff, J., Mschelia, A., Leung, T. S., Lyon, S., Marrow, J., Ganther, W. and Cole, I. S., “Atmospheric-Induced Stress Corrosion Cracking of Austenitic Stainless Steels under Limited Chloride Supply”, Paper No. 427, 18th International Corrosion Congress, 2011, Perth, Australia.Google Scholar