Liquid-Liquid Phase Separation and Phase Diagrams of Simulated Fernald Waste Glasses

Published online by Cambridge University Press:  25 February 2011

E. Wang
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington D.C. 20064
F. Perez-Cardenas
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington D.C. 20064
H. Kuang
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington D.C. 20064
A.C. Buechele
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington D.C. 20064
Get access

Abstract

Previous study of crystallization behavior in heat-treated Fernald waste glasses has produced an extensive data base of crystal phases likely to appear in various composition ranges and their corresponding liquidus temperatures. In addition, we have frequently observed amorphous phase separation in these glasses and, occasionally, evidence of crystallization originating from such phase separation. These glasses contain more than 10 components. The composition ranges for the major components are: MgF2 10–26 wt%; CaO 4–27 wt%; Al2O3 3–15 wt%; SiO2 25–40 wt%. The morphology of the phase separation as observed in the Scanning Electron Microscope (SEM) is dark, spherical globules dispersed in a continuous matrix. Globules are depleted in Mg, Ca and F, and enriched in Al and Si compared to the matrix. Phase separation occurs more frequently in melts relatively higher in Si and F. A more systematic study on a simplified and simulated seven component system (Al2O3, B2O3, CaO, Fe2O3, SiO2, Na2O and MgF2) has been undertaken to determine the subliquidus miscibility gap and liquidus curve data. Glasses were formulated by varying the concentrations of MgF2, CaO, Al2O3 and SiO2 within the ranges specified above at fixed levels of Fe2O3, B2O3 and Na2O. The miscibility gap and liquidus curve were obtained by heat-treating the glass samples at different temperatures and observing any phase separation and crystallization in the SEM and the Transmission Electron Microscope (TEM). We report here the results of this study to enhance the understanding of the thermodynamic properties of multi-component silicate systems which are usually the basis of nuclear waste glasses.

Type
Research Article
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Pegg, I.L., in Mixed Waste-Proceedings of the Second International Symposium, edited by Moghissi, A.A., Blauvelt, R.K., Benda, G.A. and Rothermich, N.E. (1993), p. 16.5.Google Scholar
2 Wang, E., Buechele, A.C., Fu, S.S. and Macedo, P.B., in Mixed Waste-Proceedings of the Second International Symposium, edited by Moghissi, A.A., Blauvelt, R.K., Benda, G.A. and Rothermich, N.E. (1993), p. 4.1.Google Scholar
3 Buechele, A.C., Wang, E. and Fu, S.S., in Ceramic Transaction-Environmental and Waste Management Issues in the Ceramic Industry. Proceedings of the 95 th Annual Meeting, American Ceramic Society (1993)(in press).Google Scholar
4 Ershova, Z.P., Geokhimiya, 4, 303 (1957).Google Scholar
5 Savva, M.A. and Newns, G.R. in Proc. IX Int. Congress on Glass, 1, 419 (1971).Google Scholar