Hostname: page-component-7f7b94f6bd-vvt5l Total loading time: 0.358 Render date: 2022-06-29T04:16:43.688Z Has data issue: true Feature Flags: { "shouldUseShareProductTool": true, "shouldUseHypothesis": true, "isUnsiloEnabled": true, "useRatesEcommerce": false, "useNewApi": true } hasContentIssue true

Article contents

Porous Ti–Al Intermetallic Based Alloys Fabricated by Pressure-Sintering Elemental Powders with a Space Holder Powder

Published online by Cambridge University Press:  30 January 2017

Naoki Takata*
Affiliation:
Dept. Materials Science and Engineering, Nagoya University, Nagoya, 464-8603, Japan
Keisuke Uematsu
Affiliation:
Dept. Materials Science and Engineering, Nagoya University, Nagoya, 464-8603, Japan
Makoto Kobashi
Affiliation:
Dept. Materials Science and Engineering, Nagoya University, Nagoya, 464-8603, Japan
Get access

Abstract

In the present study, we have attempted to produce the porous Ti–Al intermetallic based alloys by pressure-sintering of the elemental powders of Ti and Al through a combustion reaction, with a NaCl space holder to achieve the development of a highly porous structure. The powders of Ti (particle size: <45 μm) and Al (particle size: <45 μm) were mixed to various total compositions of Ti–0-40 Al (at.%), and NaCl (particle size: 300-400 μm) was mixed with the Ti/Al powder to give a highly porous structure. The mixed powder was sintered at 700 oC under a constant pressure of 30 MPa to form cylindrical specimens with a diameter of 20 mm. The soaking of the specimens in pure water allows for the removal of NaCl (with a volume fraction of 60 %) and the formation of the pores to achieve a controlled relative density of 0.4. The present process can produce porous Ti–Al alloys with various compositions. In as-sintered Ti–Al specimens, an inhomogeneous microstructure consisting of Ti particles surrounded by the a Ti–Al alloy layer (various Ti–Al intermetallic phases) was observed. The as-sintered specimens exhibited the brittle behavior under compression, which is independent of their Al content. However, in a Ti–20Al alloy heat-treated at 1300 °C, a nearly Ti3Al single-phase microstructure appeared in the porous specimen. The heat-treated porous Ti–20Al alloy shows both a high plateau-strength level of approximately 100 MPa and a high plateau-end strain over 50%, resulting in a high absorption energy. The present results demonstrate that controlling the microstructure for the formation of the Ti3Al single-phase would be an effective method to achieve high energy absorption capacity of the porous Ti–Al alloy.

Type
Articles
Copyright
Copyright © Materials Research Society 2017 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Ashby, M. F., Evans, A., Fleck, N. A., Hutchinson, J. W., Wadley, H.N.G., Metals Foams : A Design Guide, Elsevier Science (2000).
Banhart, J., Prog. Mater. Sci. 46, 559 (2001).CrossRef
Lefebvre, L.-P., Banhart, J. and Dunand, D., Adv. Eng. Mater. 10, 775 (2008).CrossRef
Banhart, J., Adv. Eng. Mater. 15, 82 (2013) .CrossRef
Koza, E., Leonowicz, M., Wojciechowski, S., Simancik, F., Mater. Let. 58, 132 (2003).CrossRef
Kanetake, N., Kobashi, M., Journal of The Japan Institute of Light Metals 62, 122 (2012).
Lasalmonie, A., Intermetallics, 14 1123 (2006).CrossRef
Wu, X., Intermetallics 14 1114 (2006).CrossRef
Gaillard, C., Despois, J. F., Mortensen, A., Mater. Sci. Eng. A 374, 250 (2004).CrossRef
Torres, Y., Pavon, J. J., Rodriguez, J. A., J Mater. Proc. Tech. 212, 1061 (2012).CrossRef
Wenjuan, N., Chenguang, B., GuiBao, Q., Qiang, W., Mater. Sci. Eng. A 506, 148 (2009).
Kobashi, M., Miyake, S., Kanetake, N., Intermetallics 42, 32 (2013).CrossRef
Kobashi, M., Inoguchi, N., Kanetake, N., Intermetallics 18, 1039 (2010).CrossRef
Arakawa, Y., Kobashi, M., Kanetake, N., Intermetallics 41, 22 (2013).CrossRef
Mansourighasri, A., Muhamad, N., Sulong, A.B., J. Mater. Proc. Tech. 212, 83 (2012).CrossRef
Liu, Y., Li, S., Hou, W., Wang, S., Hao, Y., Yang, R., Sercombe, T. B., Zhang, L.-C., J. Mater. Sci. Tech. 32, 505 (2016).CrossRef
Jha, N., Mondal, D.P., Majumdar, J. D, Badkul, A., Jha, A.K., Khare, A.K., Materials and Design 47, 810 (2013).CrossRef
Lipsitt, H. A., Shechtman, D. S., Schafrik, R. E., Metall. Trans. A 11, 1369 (1980).CrossRef
Inui, H., Toda, Y., Shirai, Y., Yamaguchi, M., Philos. Mag. A 69, 1161(1994).CrossRef
Minonishi, Y., Philos. Mag. A 63, 1085 (1991).CrossRef
Umakoshi, Y., Nakano, T., Ogawa, B., Scr. Mater. 34, 1161 (1996).CrossRef
Naruse, W., Kondo, S., Kobashi, M., Kanetake, N., Iwata, Y., Nishiwaki, T., Journal of The Japan Institute of Light Metals 64, 598 (2014).CrossRef

Save article to Kindle

To save this article to your Kindle, first ensure coreplatform@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Porous Ti–Al Intermetallic Based Alloys Fabricated by Pressure-Sintering Elemental Powders with a Space Holder Powder
Available formats
×

Save article to Dropbox

To save this article to your Dropbox account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you used this feature, you will be asked to authorise Cambridge Core to connect with your Dropbox account. Find out more about saving content to Dropbox.

Porous Ti–Al Intermetallic Based Alloys Fabricated by Pressure-Sintering Elemental Powders with a Space Holder Powder
Available formats
×

Save article to Google Drive

To save this article to your Google Drive account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you used this feature, you will be asked to authorise Cambridge Core to connect with your Google Drive account. Find out more about saving content to Google Drive.

Porous Ti–Al Intermetallic Based Alloys Fabricated by Pressure-Sintering Elemental Powders with a Space Holder Powder
Available formats
×
×

Reply to: Submit a response

Please enter your response.

Your details

Please enter a valid email address.

Conflicting interests

Do you have any conflicting interests? *