Correlated Post-mortem Raman and TEM Investigation of Nanoindentation Induced Structural Changes in Silicon as a Function of Temperature
Published online by Cambridge University Press: 30 July 2020
Abstract
An abstract is not available for this content so a preview has been provided. As you have access to this content, a full PDF is available via the ‘Save PDF’ action button.
![Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'](https://static.cambridge.org/content/id/urn%3Acambridge.org%3Aid%3Aarticle%3AS143192762002245X/resource/name/firstPage-S143192762002245Xa.jpg)
- Type
- Surface and Subsurface Microscopy and Microanalysis of Physical and Biological Specimens
- Information
- Copyright
- Copyright © Microscopy Society of America 2020
References
Weinstein, B. A., & Piermarini, G. J. (1975). Raman scattering and phonon dispersion in Si and GaP at very high pressure. Physical Review B, 12(4), 1172.10.1103/PhysRevB.12.1172CrossRefGoogle Scholar
Minomura, S., & Drickamer, H. G. (1962). Pressure induced phase transitions in silicon, germanium and some III–V compounds. Journal of Physics and Chemistry of Solids, 23(5), 451–456.10.1016/0022-3697(62)90085-9CrossRefGoogle Scholar
Jamieson, J. C. (1963). Crystal structures at high pressures of metallic modifications of silicon and germanium. Science, 139(3556), 762–764.10.1126/science.139.3556.762CrossRefGoogle ScholarPubMed
Gerbig, Y. B., Michaels, C. A., Forster, A. M., & Cook, R. F. (2012). In situ observation of the indentation-induced phase transformation of silicon thin films. Physical Review B, 85(10), 104102.10.1103/PhysRevB.85.104102CrossRefGoogle Scholar
Domnich, V., Aratyn, Y., Kriven, W. M., & Gogotsi, Y. (2008). Temperature dependence of silicon hardness: experimental evidence of phase transformations. Rev. Adv. Mater. Sci, 17(1-2), 33–41.Google Scholar