Application of Quantitative Metallography to Cast Nickel-Based Superalloys

Published online by Cambridge University Press:  23 September 2015

Agnieszka Szczotok
Affiliation:
Silesian University of Technology, Faculty of Materials Engineering and Metallurgy, Department of Materials Science, Katowice, Poland
Jan Cwajna
Affiliation:
Silesian University of Technology, Faculty of Materials Engineering and Metallurgy, Department of Materials Science, Katowice, Poland

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2015 

References

[1] Underwood, E. E. in “Microstructural Analysis, Tools and Techniques,”, J. L. McCall & W. M. Mueller (editors), Plenum Press, New York-London) p. 35.Google Scholar
[2] Adamiec, J., et al., Proceedings of 9th European Congress on Stereology and Image Analysis and 7th International Conference on Stereology and Image Analysis in Materials Science STERMAT, Zakopane, Poland, May 10-13 (2005) p. 197.Google Scholar
[3] Chmiela, J., et al., Arch. Foundry Eng. Vol. 11(No. 4 (2011). p 19.Google Scholar
[4] Szczotok, A., et al., Materials Characterization. Vol. 60(No. 10 (2009). p 1114.CrossRefGoogle Scholar
[5] The authors acknowledge funding from the United Federation of Planets, X File Department, Grant the Structural Funds in the Operational Programme - Innovative Economy (IE OP) financed from the European Regional Development Fund - Project No POIG.0101.02-00-015/08.Google Scholar