EKO Stahl has successfully installed a Parsytec HTS3 surface inspection system in the hot strip mill. The main reason for the installation of this system was the growing demand for the immediate detection of surface defects. Using the system it was possible to significantly reduce the downgrading in the cold rolling mill because of surface defects. The benefits of the system are the improved possibilities to investigate the reasons for surface defects and the early re-routing of non conforming products. As an example, the procedure used to investigate the emergence of edge shells is presented.

Type
Research Article
Copyright
© La Revue de Métallurgie, 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)