Hostname: page-component-78c5997874-j824f Total loading time: 0 Render date: 2024-11-17T19:37:20.375Z Has data issue: false hasContentIssue false

Orientation-dependent properties of silicon nitride with aligned reinforcing grains

Published online by Cambridge University Press:  31 January 2011

Dong-Soo Park
Affiliation:
Ceramic Materials Group, Korea Institute of Machinery and Materials, 66 Sang-Nam-Dong, Chang-Won City, Kyong-Nam, South Korea
Myoung-Je Choi
Affiliation:
Ceramic Materials Group, Korea Institute of Machinery and Materials, 66 Sang-Nam-Dong, Chang-Won City, Kyong-Nam, South Korea
Tae-Wook Roh
Affiliation:
Ceramic Materials Group, Korea Institute of Machinery and Materials, 66 Sang-Nam-Dong, Chang-Won City, Kyong-Nam, South Korea
Hai-Doo Kim
Affiliation:
Ceramic Materials Group, Korea Institute of Machinery and Materials, 66 Sang-Nam-Dong, Chang-Won City, Kyong-Nam, South Korea
Byung-Dong Han
Affiliation:
Ceramic Materials Group, Korea Institute of Machinery and Materials, 66 Sang-Nam-Dong, Chang-Won City, Kyong-Nam, South Korea
Get access

Extract

Silicon nitride with the aligned reinforcing grains was prepared by tape casting with addition of the silicon nitride whiskers and gas-pressure sintering at 2148 K. The microstructure and the mechanical properties of the sintered sample, including the fracture toughness and the three-point flexural strength, were highly anisotropic. Both the fracture toughness and the flexural strength were the highest when the crack-propagation direction was normal to the alignment direction. This result was interpreted from the laminate composite materials’ point of view. Although the large elongated grains were as long as 44.4 ± 12 μm and as wide as 5.1 ± 0.67 μm, they were not the fracture origins.

Type
Articles
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1.Becher, P.F., J. Am. Ceram. Soc. 74, 255 (1991).CrossRefGoogle Scholar
2.Ferber, K.T. and Evans, A.G., Acta Metall. 31, 577 (1983).Google Scholar
3.Sajgalik, P., Dusza, J., and Hoffmann, M.J., J. Am. Ceram. Soc. 78, 2619 (1995).CrossRefGoogle Scholar
4.Hirao, K., Ohashi, M., Britio, M.E., and Kanzaki, S., J. Am. Ceram. Soc. 78, 1687 (1995).CrossRefGoogle Scholar
5.Becher, P.F., Sun, E.Y., Plucknett, K.P., Alexander, K.B., Hsueh, C-H., Waters, S.B., Westmoreland, C.G., Kang, E-S., Hirao, K., and Brito, M.E., J. Am. Ceram. Soc. 81, 2821 (1998).CrossRefGoogle Scholar
6.Ohji, T., Hirao, K., and Kanzaki, S., J. Am. Ceram. Soc. 78, 3125 (1995).CrossRefGoogle Scholar
7.Evans, A.G. and Charles, E.A., J. Am. Ceram. Soc. 59, 371 (1976).CrossRefGoogle Scholar
8.Mücklich, F., Ohser, J., Hartmann, S., Hoffmann, M.J., and Petzow, G., in Tailoring of Mechanical Properties of Si3N4 Ceramics, NATO ASI Series, Series E, Applied Science Vol. 276, edited by Hoffmann, M.J. and Petzow, G. (Kluwer Academic Publishers, Dordrecht, The Netherlands, 1994), pp. 7386.CrossRefGoogle Scholar
9.Li, C-W., Lui, S-C., and Goldacker, J., J. Am. Ceram. Soc. 78, 449 (1995).CrossRefGoogle Scholar
10.Warren, R. and Sarin, V.K., in Application of Fracture Mechanics to Composite Materials, Composite Materials Series Vol. 6, edited by Freidrich, K. (Elsevier, Amsterdam, The Netherlands, 1989), p. 571.CrossRefGoogle Scholar
11.Barrett, C.R., Nix, W.D., and Tetelman, A.S., The Principles of Engineering Materials (Prentice-Hall, Englewood, NJ, 1973), p. 316.Google Scholar