Study of The Quasicrystal Formation in Zr46.8Ti8.2Cu7.5Ni10Be27.5 Bulk Metallic Glass

Published online by Cambridge University Press:  11 February 2011

J.L. Soubeyroux
Affiliation:
Laboratoire de Cristallographie/CRETA/ CNRS, 25 avenue des Martyrs, 38042 Grenoble, France
J.M. Pelletier
Affiliation:
GEMPPM, INSA Lyon, bâtiment B. Pascal, 20 Avenue A.Einstein, 69621 Villeurbanne, France
B. Van de Moortèle
Affiliation:
GEMPPM, INSA Lyon, bâtiment B. Pascal, 20 Avenue A.Einstein, 69621 Villeurbanne, France
T. Epicier
Affiliation:
GEMPPM, INSA Lyon, bâtiment B. Pascal, 20 Avenue A.Einstein, 69621 Villeurbanne, France
Get access

Abstract

The formation of the primary crystals appearing during isothermal annealing of the Zr46.8Ti8.2Cu7.5Ni10Be27.5 (Vit4) bulk metallic glasses has been studied by in-situ neutron diffraction, DSC, high resolution TEM and electron diffraction. We have evidenced that the primary phase appearing on the isothermal plateau at 620 K is quasicrystalline and is beryllium free. Moreover, we have prepared an alloy with the composition determined by EDX (without beryllium), and studied the formation of quasicrystals in this alloy. A comparison is done between the quasicrystalline phases appearing during the annealing of Vit4 and the quasicrystals prepared without beryllium in an amorphous alloy prepared by melt spinning. In particular they have the same intensities and peak positions in the diffraction studies.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Johnson, W.L., Mater. Sci. Forum 225–227 (1996) 35; MRS Bull. 24 (1999) 42Google Scholar
[2] Löffler, J.F. and Johnson, W.L., Mat. Sci. Eng. A 304–306 (2001) 670; Scripta mater. 44 (2001) 1251Google Scholar
[3] Wanderka, N., Macht, M.-P., Seidel, M., Mechler, S., Stahl, K. and Jiang, J.Z., Appl. Phys. Lett. 77 (2000) 3935 Google Scholar
[4] Macht, M.-P., Wanderka, N., Wei, Q., Sieber, I. and Deyneka, N., Mat. Sci. Eng. A 304–306 (2001) 701 Google Scholar
[5] Poon, S.J., Drehman, A.J. and Lawless, K.R., Phys Rev. Lett. 55 (1985) 2324 Google Scholar
[6] Kelton, K.F., Kim, W.J. and Stroud, R.M., Appl. Phys. Lett. 70 (1997) 3230 Google Scholar
[7] Saida, J., Matsushita, M., Zhang, T., Inoue, A., Chen, M. and Sakurai, T., Appl. Phys. Lett. 75 (1999) 3497 Google Scholar
[8] Köster, U., Meinhardt, J., Roos, S. and Liebertz, H., Appl. Phys. Lett. 69 (1996) 179 Google Scholar
[9] Köster, U., Zander, D. and Janlewing, R., Mat. Res. Symp. Proc. Vol.644 (2001) L581 Google Scholar
[10] Pelletier, J.M., Jacquemard, Y., Perez, J. and Perrier de la Bâthie, R., Mat. Res. Symp. Proc. Vol. 554 (1999) 413 Google Scholar
[11] Van de Moortèle, B., Epicier, T., Soubeyroux, J.L. and Pelletier, J.M., submitted to Acta mater.Google Scholar
[12] Jiang, J.Z., Rasmussen, A.R., Jensen, C.H., Lin, Y. and Hansen, P.L., Appl. Phys. Lett. 80 (2003) 2090 Google Scholar
[13] Louzguine, D.V. and Inoue, A., Appl. Phys. Lett. 78 (2001) 1841 Google Scholar
[14] Ma, L., Wang, L. and Inoue, A., J. of Mat. Sci. Lett. 20 (2001) 161 Google Scholar