Excimer (XeCl) Laser Annealing of PbZr0.4Ti0.6O3 Thin Film at Low Temperature for TFT FeRAM Application

Published online by Cambridge University Press:  01 February 2011

W. X. Xianyu
Affiliation:
Samsung Advanced Institute of Technology, P.O. Box 111, Suwon 440–600, Gyunggi-Do, Korea
H. S. Cho
Affiliation:
Samsung Advanced Institute of Technology, P.O. Box 111, Suwon 440–600, Gyunggi-Do, Korea
J. Y. Kwon
Affiliation:
Samsung Advanced Institute of Technology, P.O. Box 111, Suwon 440–600, Gyunggi-Do, Korea
H.X. Yin
Affiliation:
Samsung Advanced Institute of Technology, P.O. Box 111, Suwon 440–600, Gyunggi-Do, Korea
T. Noguchi
Affiliation:
Samsung Advanced Institute of Technology, P.O. Box 111, Suwon 440–600, Gyunggi-Do, Korea Sungkyunkwan University, Suwon 440–746, Gyunggi-Do, Korea
Get access

Abstract

In this study, we successfully produced PbZr0.4Ti0.6O3 (PZT (40/60)) thin films with high crystallinity and high remnant polarization (Pr) at low process temperatures using pulsed excimer (XeCl) laser irradiation. In our experiments, amorphous PZT films were prepared on Pt/Ti/SiO2/Si substrates by a sol-gel method. A two-step process was used to crystallize the amorphous thin films: the films were annealed at 550°C for 10 min to initiate the nucleation of the PZT perovskite phase, and then annealed with an excimer laser heating at 400°C in a 120 Torr nitrogen gas atmosphere. Laser energy density was varied from 150 to 750 mJ/cm2 per pulse. x-ray diffraction (XRD) patterns show that 150–200 mJ/cm2 range multi-shot excimer laser irradiation drastically improved the crystallinity of the PZT perovskite phase, and FESEM photographs show that the PZT thin film has uniform-sized crystal grains. The ferroelectric properties were found to depend on the laser energy density and shot number. Before the laser annealing, the films show hysteresis loops with low Pr and the loops do not saturate. After laser annealing, the films show highly saturated hysteresis loops, with the Pr increasing from 2.2 μC/cm2 to 23.0 μC/cm2. We also propose a new technology for fabrication of thin film transistor (TFT)-driven FeRAM devices on arbitrary insulator substrate such as on glass.

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Noguchi, T., Kim, D.Y., Kwon, J.Y., Park, K.B., Jung, J.S., Xianyu, W.X., Yin, H.X. and Cho, H.S., Mat. Res. Soc. Symp. Proc. 814, 7 (2004)Google Scholar
2. Digest of Technical papers on AM-LCD, p. 71 (2001)Google Scholar
3. Lemmi, F., Lin, S., Drews, B.C., Hua, A., Stern, J.R., Chung, W., Smith, P.M., Chen, J.Y., Mat. Res. Soc. Symp. Proc. 814, 15 (2004)Google Scholar
4. Park, Y.S., Koo, J.M., Shin, S.M. and Kim, S.P., Tech. Dig. 2004 Asia-pacific workshop on fundamentals and application of advanced semiconductor devices, June 30-July 2. 157 (2004)Google Scholar
5. Joo, H.J., Song, Y.J., Kim, H.H., Kang, S.K., Park, J.H., Kang, Y.M., Kang, E.Y., Lee, S.Y., Jeong, H.S. and Kim, K., 2004 Symposium on VLSI technology Digest of technical papers, 148 (2004)Google Scholar
6. Zhu, Y.F., Zhu, J.S., Song, Y.J., and Desu, S.B., Appl. Phys. Lett. 73, 1958 (1958)Google Scholar
7. Lu, X.M., Zhu, J.S., Hu, W.S., Liu, Z.G., and Wang, Y.N., Appl. Phys. Lett. 66, 2481 (1995)Google Scholar
8. Chou, C.F., Pan, H.C. and Chou, C.C., Jpn. J. Appl. Phys. 41, 6679 (2002)Google Scholar
9. Pan, H.C., Chou, C.C., and Tsai, H.L., Appl. Phys. Lett. 83, 3156 (2003)Google Scholar
10. Shye, D.C., Chiou, B.S., Hwang, C.C., Jaing, C.C., Hsu, H.W., Chen, J.S. and Cheng, H.C., Jpn. J. Appl. Phys. 42, 1680 (2003)Google Scholar