Epitaxial Growth of Highly Crystallized InSb films on Si Substrate by MBE and Their Devices Properties

Published online by Cambridge University Press:  31 January 2011

Yoshihisa Kunimi
Affiliation:
kunimi.yb@om.asahi-kasei.co.jp, Asahi Kasei Microdevices Corporation, Magnetic Sensor Process Technology & Development, Fuji, Japan
Hiromi Fujita
Affiliation:
fujita.hcc@om.asahi-kasei.co.jp, Asahi Kasei Microdevices Corporation, Magnetic Sensor Process Technology & Development, Fuji, Japan
Ayano Sakurai
Affiliation:
sakurai.ab@om.asahi-kasei.co.jp, Asahi Kasei Microdevices Corporation, Magnetic Sensor Process Technology & Development, Fuji, Japan
Shinichiro Akiyama
Affiliation:
akiyama.sm@om.asahi-kasei.co.jp, Asahi Kasei Microdevices Corporation, Magnetic Sensor Process Technology & Development, Fuji, Japan
Masatoshi Miyahara
Affiliation:
miyahara.mb@om.asahi-kasei.co.jp, Asahi Kasei Microdevices Corporation, Magnetic Sensor Process Technology & Development, Fuji, Japan
Yoshihiko Shibata
Affiliation:
shibata.yk@om.asahi-kasei.co.jp, Asahi Kasei Microdevices Corporation, Magnetic Sensor Process Technology & Development, Fuji, Japan
Get access

Abstract

High crystallized thin InSb epitaxial growth directly on Si substrate was investigated by molecular-beam epitaxy (MBE). Experimental results indicated that suppressing the desorption of hydrogen atoms which terminated the dangling bonds of Si wafer surface and incorporation of As around the interface between film and Si substrate were the most important to obtained high crystallized InSb film. It could be achieved by the irradiation of As4 cluster beam onto the Si wafer just before film growth. Obtained thin InSb film showed mirror like surface, and its thickness was 0.7 μm. Its electron mobility was 47,600 cm2/V-s, and FWHM of HR-XRD rocking curve was about 300 arcsec. This InSb film on Si wafer was applied to Hall element, and it passed ordinary reliability tests.

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Datta, S., et.al. IEDM Tech. Digest. 783786 (2005)Google Scholar
[2] Li, L.K., et al., J. Vac. Sci. Technol. B, 11(3) 872–87 (1993)10.1116/1.586769Google Scholar
[3] Chyi, J.-I., et. al., 54(11), 10161018 (1989)Google Scholar