Hostname: page-component-76fb5796d-zzh7m Total loading time: 0 Render date: 2024-04-25T10:54:39.333Z Has data issue: false hasContentIssue false

Corrosion of K-3 Glass-contact refractory in sodium-rich aluminosilicate melts

Published online by Cambridge University Press:  10 February 2011

X. D. Lu
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064.
H. Gan
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064.
A. C. Buechele
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064.
I. L. Pegg
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064.
Get access

Abstract

The corrosion of the glass-contact refractory Monofrax K-3 in two sodium-rich aluminosilicate melts has been studied at 1208 and 1283°C using a modified ASTM procedure with constant agitation of the melt by air bubbling. The results for the monolithic refractory indicate a fast initial stage involving phase dissolution and transformation and a later “passivated” stage in which the surface of the refractory has been substantially modified. The composition of the stable spinel phase in the altered layer on monolithic coupons of K-3 is almost identical to the equilibrium composition bracketed by the dissolution of powdered K-3 into under-saturated melts on the one hand, and by crystallization of spinels from supersaturated melts on the other. The temperature and melt shear viscosity were found to have significant effects on the rates of K-3 dissolution and transformation.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Bickford, D. F., Ondrejcin, R. S., Salley, L., "High-Temperature Materials for Radioactive Waste Incineration and Vitrification," Advances in Ceramics, Nuclear Waste Management II 20 p. 65 (1986).Google Scholar
[2] Xing, S. B., Lin, Y., Mohr, R. K., and Pegg, I. L., "Corrosion Resistance of Ceramic Refractories to Simulated Waste Glasses at High Temperatures," Scientific Basis for Nuclear Waste Management XIX, Eds. Murphy, W. M. and Knecht, D. A., MRS, Pittsburgh, PA, 412, 181 (1996).Google Scholar
[3] Wang, E., Mohr, R. K., Buechele, A. C., and Pegg, I. L., "Current Density Effects on the Corrosion of Ceramic and Metallic Electrode Materials in Waste Glasses," Scientific Basis for Nuclear Waste ManagementXIX, Eds. Murphy, W. M. and Knecht, D. A., MRS, Pittsburgh, PA, 412 181 (1996).Google Scholar
[4] Buchele, A. C., Fu, S. S., Yan, Q., and Pegg, I. L., "Radionuclide Uptake by Waste Glass Melter Refractories," Environmental Issues and Waste Management Technologies in the Ceramic and Nuclear Industries III, Eds. Peeler, D.K. and Marra, J.C., Ceramic Transactions, 87, p. 583 (1998).Google Scholar
[5] Muller, I. S., Buechele, A. C., Perez-Cardenas, F., Gan, H., and Pegg, I. L., "Partitioning of Plutonium Between Glass, Secondary Phases, and Contract Refractories," Materials Research Society, these Proceedings.Google Scholar