Hostname: page-component-79b67bcb76-kmcbj Total loading time: 0.136 Render date: 2021-05-15T18:19:26.605Z Has data issue: true Feature Flags: { "shouldUseShareProductTool": true, "shouldUseHypothesis": true, "isUnsiloEnabled": true, "metricsAbstractViews": false, "figures": false, "newCiteModal": false, "newCitedByModal": true, "newEcommerce": true }

Defect Evolution During Laser Annealing

Published online by Cambridge University Press:  01 February 2011

Susan B. Felch
Affiliation:
susan_felch@amat.com, Applied Materials, Front End Products Group, 974 E. Arques Avenue, M/S 81280, Sunnyvale, CA, 94085, United States, 408-584-1273, 408-584-1194
Abhilash Mayur
Affiliation:
abhilash_mayur@amat.com, Applied Materials, Front End Products Group, 974 E. Arques Avenue, Sunnyvale, CA, 94085, United States
Vijay Parihar
Affiliation:
vijay_parihar@amat.com, Applied Materials, Front End Products Group, 974 E. Arques Avenue, Sunnyvale, CA, 94085, United States
Faran Nouri
Affiliation:
faran_nouri@amat.com, Applied Materials, Front End Products Group, 974 E. Arques Avenue, Sunnyvale, CA, 94085, United States
Kevin S. Jones
Affiliation:
kjones@eng.ufl.edu, University of Florida, Dept. of Materials Science, Gainesville, FL, 32611, United States
Daniel E. Zeenberg
Affiliation:
dzgator@ufl.edu, University of Florida, Dept. of Materials Science, Gainesville, FL, 32611, United States
Britta E. Jones
Affiliation:
brittae@ufl.edu, University of Florida, Dept. of Materials Science, Gainesville, FL, 32611, United States
Get access

Abstract

Implementation of millisecond annealing requires the identification of the operating conditions for that technique which minimize the residual defects. In addition, possible combinations of low temperature annealing with millisecond annealing could result in minimal residual defects. The samples studied here were implanted with Ge+ pre-amorphization and boron dopant ions and were activated with a scanning laser annealing technique with maximum temperature dwell times of about one millisecond. The laser anneal conditions were varied, along with combinations of spike anneals. The annealed samples were analyzed by plan-view transmission electron microscopy (TEM) to measure the residual defect density and size. The effects of spike temperature, laser annealing temperature, and scan rate will be discussed.

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below.

References

1 The International Technology Roadmap for Semiconductors, 2005.Google Scholar
2 Noda, T., Felch, S., Parihar, V., Vrancken, C., Janssens, T., and Vandervorst, W., submitted to These Proceedings.Google Scholar
3 Zeenberg, D. and Jones, K., submitted to These Proceedings.Google Scholar
4 Ostwald, W., Z. Phys. Chem., Stoechiom. Verwandtschaftsl. 34, 495 (1900).Google Scholar
5 Burton, B. and Speight, M. V., Philos. Mag. A 53, 385 (1986).CrossRefGoogle Scholar
6 Jain, A., Mat. Res. Soc. Symp. Proc., Vol. 810, p. 229 (2004).CrossRefGoogle Scholar
7 Felch, S.B., Graoui, H. and Mayur, A., Proc. of Intl. Symp. On Advanced Short-Time Thermal Processing for Si-Based CMOS Devices II, Electrochemical Society, Vol. 2004–01, p. 31.Google Scholar
8 Falepin, A., Janssens, T., Severi, S., Vandervorst, W., Felch, S.B., Parihar, V., and Mayur, A., Proc. of 2005 RTP Conference, IEEE.Google Scholar
9 Jacques, J. M., presentation at Spring 2004 Materials Research Society symposium.Google Scholar

Send article to Kindle

To send this article to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about sending to your Kindle. Find out more about sending to your Kindle.

Note you can select to send to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be sent to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Defect Evolution During Laser Annealing
Available formats
×

Send article to Dropbox

To send this article to your Dropbox account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Dropbox.

Defect Evolution During Laser Annealing
Available formats
×

Send article to Google Drive

To send this article to your Google Drive account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Google Drive.

Defect Evolution During Laser Annealing
Available formats
×
×

Reply to: Submit a response


Your details


Conflicting interests

Do you have any conflicting interests? *