Hostname: page-component-65dc7cd545-nrv4r Total loading time: 0.227 Render date: 2021-07-24T18:06:37.075Z Has data issue: true Feature Flags: { "shouldUseShareProductTool": true, "shouldUseHypothesis": true, "isUnsiloEnabled": true, "metricsAbstractViews": false, "figures": true, "newCiteModal": false, "newCitedByModal": true, "newEcommerce": true, "newUsageEvents": true }

Model Materials for Irradiated Fuels: Study of Local Mechanical Behavior Using Nanoindentation and Microstructural Analysis

Published online by Cambridge University Press:  27 August 2014

Nathalie Payraudeau Le Roux
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Sylvain Meille
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Cyril Langlois
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Isabelle Zacharie-Aubrun
Affiliation:
CEA, DEN, DEC Cadarache, 13108 St Paul Lez Durance, France
Thierry Douillard
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Jean-Marie Gatt
Affiliation:
CEA, DEN, DEC Cadarache, 13108 St Paul Lez Durance, France
Rights & Permissions[Opens in a new window]

Abstract

Image of the first page of this article. For PDF version, please use the ‘Save PDF’ preceeding this image.
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2014 

References

[1] Anstis, G. R, et al. (1981), Journal of the American Ceramic Society, 64:533-538.CrossRef
[2] Dukino, R. D, et al. (1992), Journal of the American Ceramic Society, 75: 3299-3304.CrossRef
You have Access

Send article to Kindle

To send this article to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about sending to your Kindle. Find out more about sending to your Kindle.

Note you can select to send to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be sent to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Model Materials for Irradiated Fuels: Study of Local Mechanical Behavior Using Nanoindentation and Microstructural Analysis
Available formats
×

Send article to Dropbox

To send this article to your Dropbox account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Dropbox.

Model Materials for Irradiated Fuels: Study of Local Mechanical Behavior Using Nanoindentation and Microstructural Analysis
Available formats
×

Send article to Google Drive

To send this article to your Google Drive account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Google Drive.

Model Materials for Irradiated Fuels: Study of Local Mechanical Behavior Using Nanoindentation and Microstructural Analysis
Available formats
×
×

Reply to: Submit a response

Please enter your response.

Your details

Please enter a valid email address.

Conflicting interests

Do you have any conflicting interests? *