Hostname: page-component-788cddb947-55tpx Total loading time: 0 Render date: 2024-10-13T15:28:05.735Z Has data issue: false hasContentIssue false

From Hardness Testing Relying on Optical Imaging to Quantitative In-Situ Nanoindentation in a Transmission Electron Microscope

Published online by Cambridge University Press:  31 July 2006

OL Warren
Affiliation:
Hysitron,Inc.
SA S Asif
Affiliation:
Hysitron,Inc.
AM Minor
Affiliation:
Lawrence Berkeley National Laboratory
Z Shan
Affiliation:
Lawrence Berkeley National Laboratory
EA Stach
Affiliation:
Purdue University
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2006 in Chicago, Illinois, USA, July 30 – August 3, 2006