Hostname: page-component-788cddb947-2s2w2 Total loading time: 0 Render date: 2024-10-18T10:53:11.275Z Has data issue: false hasContentIssue false

Characterization of Nanoindentations in Silicon by Cross-sectional TEM

Published online by Cambridge University Press:  01 August 2004

Songqing Wen
Affiliation:
University of Tennessee
James Bentley
Affiliation:
Oak Ridge National Laboratory, Tennessee
Jae-il Jang
Affiliation:
University of Tennessee
Ian M. Anderson
Affiliation:
Oak Ridge National Laboratory, Tennessee
George M. Pharr
Affiliation:
University of Tennessee Oak Ridge National Laboratory, Tennessee
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2004 in Savannah, Georgia, USA, August 1–5, 2004.