Stabilization of lead lithium iron tungstate with adding barium titanate

Published online by Cambridge University Press:  31 January 2011

Chung-Hsin Lu
Affiliation:
Department of Chemical Engineering, National Taiwan University, Taipei, Taiwan, Republic of China
Buh-Kuan Fang
Affiliation:
Department of Chemical Engineering, National Taiwan University, Taipei, Taiwan, Republic of China
Get access

Abstract

The kinetics of formation, phase stabilities, and dielectric constants of Pb(Li1/4Fe1/4W1/2)O3 and BaTiO3-added Pb(Li1/4Fe1/4W1/2)O3 have been compared. The addition of 2 mol% BaTiO3 in Pb(Li1/4Fe1/4W1/2)O3 was confirmed to promote the complete formation of the perovskite phase at 700 °C. Also, the thermal stability of the perovskite phase was significantly enhanced, which resulted in an increase of the dielectric permittivity.

Type
Articles
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1.Lejeune, M. and Boilot, J. P., Mater. Res. Bull. 20, 493 (1985).CrossRefGoogle Scholar
2.Chen, C. F. and Fu, S. F., J. Mater. Sci. 25, 424 (1990).CrossRefGoogle Scholar
3.Viskov, A. S., Venevstev, Yu. N., Zhdanov, G. S., and Onikienko, L. D., Sov. Phys. Crystallogr. 10, 720 (1966).Google Scholar
4.Shvornea, L. I., Venevstev, Yu. N., and Zhdanov, G. S., Inorg. Mater. 2, 1602 (1966).Google Scholar
5.Lu, C. H. and Hwang, W. S., J. Ceram. Soc. Jpn. 104, 587 (1996).CrossRefGoogle Scholar
6.Sakata, K. and Takahara, H., Jpn. J. Appl. Phys. 26, Suppl. 26–2, 83 (1987).CrossRefGoogle Scholar
7.Lu, C. H. and Hwang, W. S., J. Mater. Res. 10, 2755 (1995).CrossRefGoogle Scholar
8.Halliyal, A., Kumar, U., Newnham, R. E., and Cross, L. E., Am. Ceram. Soc. Bull. 66, 671 (1987).Google Scholar
9.Halliyal, A., Kumar, U., Newnham, R. E., and Cross, L. E., J. Am. Ceram. Soc. 70, 119 (1987).CrossRefGoogle Scholar
10.Kang, D. H. and Yoon, K. H., J. Mater. Sci. 26, 56 (1991).CrossRefGoogle Scholar
11.Sakurai, O., Katsumoto, M., Shinozaki, K., and Mizutani, N., J. Ceram. Soc. Jpn. 101, 607 (1993).CrossRefGoogle Scholar