Corrosion barriers for silver-based telescope mirrors comparing PEALD and PVD of AlOx

Published online by Cambridge University Press:  13 July 2015

David M. Fryauf
Affiliation:
Baskin School of Engineering, University of California Santa Cruz, Santa Cruz, CA 95064, USA
Andrew C. Phillips
Affiliation:
University of California Observatories, Univ. of California, Santa Cruz, CA, USA 95064
Nobuhiko P. Kobayashi
Affiliation:
Nanostructured Energy Conversion Technology and Research (NECTAR), Advanced Studies Laboratories, Univ. of California Santa Cruz – NASA Ames Research Center, Moffett Field, CA 94035, USA
Get access

Abstract

Astronomical telescopes continue to demand high-endurance high-reflectivity silver mirrors that can withstand years of exposure in earth-based observatory environments. The University of California Observatories Astronomical Coatings Lab has undertaken development of protected silver coatings suitable for telescope mirrors that maintain high reflectivity at wavelengths from 340 nm through the mid-infrared spectrum. We present promising results of enhanced corrosion barriers using plasma-enhanced atomic layer deposition (PEALD) of aluminum oxide (AlOx) as a top barrier layer. Novel coating recipes developed with ion-assisted electron beam deposition (IAEBD) of materials including yttrium fluoride and oxides of yttrium, tantalum, and silicon are used to compare the endurance of physical vapor deposition-grown barriers with PEALD-grown barriers of similar thickness. Samples of these mirror coatings were covered with conformal layers of AlOx deposited by PEALD using trimethylaluminum as a metal precursor and plasma-activated oxygen as an oxidant gas. Samples of coating recipes with and without PEALD oxide undergo aggressive high temperature/high humidity (HTHH) environmental testing in which samples are exposed to an environment of 80% humidity at 80°C for ten days in a simple test set-up. HTHH testing show visible results suggesting that the PEALD oxide offers enhanced robust protection against chemical corrosion and moisture from an accelerated aging environment. Mirror samples are further characterized by reflectivity/absorption before and after deposition of oxide coatings. AlOx is suitable for many applications and has been the initial material choice for this study.

Type
Articles
Copyright
Copyright © Materials Research Society 2015 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Jacobson, M. R., Kneale, R., Raybould, K., Gillett, F. C., Laird, R., Shimshock, R. P., and Booth, D. C., Proc. SPIE 3352, 477502 (1998).CrossRefGoogle Scholar
Boccas, M., Vucina, T., Araya, C., Esteban, V., and Ahhee, C., Proc. SPIE 5494, 239 (2004).CrossRefGoogle Scholar
Vucina, T., Boccas, M., Araya, C., Ah Hee, C., and Cavedoni, C., Proc. SPIE 7012, 70122Q1 (2008).CrossRefGoogle Scholar
Phillips, A. C., Miller, J., Brown, W. E., Hilyard, D., DuPraw, B., Wallace, V., and Cowley, D., Proc. SPIE 7018, 70185A (2008).CrossRefGoogle Scholar
Phillips, A. C., Brown, W. E., DuPraw, B., Hilyard, D. F., and Cowley, D. J., Proc. SPIE 7739, 77393Y (2010).CrossRefGoogle Scholar
Phillips, A. C., Miller, J. S., Bolte, M., DuPraw, B., Radovan, M. V., and Cowley, D. J., Proc. SPIE 8450, 84502G (2012).Google Scholar
Martin, P. J., Journal of materials science 21, 1, 125 (1986).CrossRefGoogle Scholar
Groner, M. D., Fabreguette, F. H., Elam, J. W., and George, S. M., Chemistry of Materials 16, 4, 639645, (2004).CrossRefGoogle Scholar
Raether, H., Surface plasmons on smooth surfaces, (Springer Berlin Heidelberg, 1988).CrossRefGoogle Scholar
Phillips, A. C., Miller, J. S., Bolte, M., DuPraw, B., Radovan, M., and Cowley, D., SPIE Astronomical Telescopes+ Instrumentation, pp. 84502G-84502G. International Society for Optics and Photonics, 2012.Google Scholar
Phillips, A. C., DuPraw, B., Hilyard, D., Gavel, D., Dillon, D., and Kupke, R., SPIE Astronomical Telescopes+ Instrumentation, pp. 91515I-91515I. International Society for Optics and Photonics, 2014.Google Scholar
von Seefeld, H, Cheung, N. W., Maenpaa, M., and Nicolet, M. A., Electron Devices, IEEE Transactions on 27, 4, 873876 (1980).CrossRefGoogle Scholar
Fryauf, D. M., Phillips, A. C., and Kobayashi, N. P., SPIE NanoScience+ Engineering, pp. 88200Y-88200Y. International Society for Optics and Photonics, 2013.Google Scholar