Instrumented nanoindentation and scanning electron transmission microscopy applied to the study of the adhesion of InP membranes heteroepitaxially bonded to Si

  • Konstantinos Pantzas (a1) (a2), Eric Le Bourhis (a2), Gilles Patriarche (a1), Ahmad Itawi (a1), Grégoire Beaudoin (a1), Isabelle Sagnes (a1) and Anne Talneau (a1)...

Abstract

Instrumented nanoindentation and STEM have been combined ex situ to study the adhesion of 450 nm thick InP membranes to Si substrates. Three distinct regimes are identified in the deformation of the InP/Si stacks during these experiments: the first is plastic flow of InP at low loads; the second is elastic debonding of the InP membrane, far from the indented zone at medium loads; lastly, the local amorphisation of the underlying Si substrate at high loads. The regime of intermediate loads is shown to be particularly useful in the evaluation of the surface bonding energy of InP to Si.

Copyright

Corresponding author

References

Hide All
[1] Roelkens, G., Broukaert, J., Van Thourhout, D., Baets, R., Notzel, R., Smit, M., J. Electrochem. Soc. 153, G1015 (2006)
[2] Lamponi, M., Keyvaninia, S., Jany, C., Poingt, F., Lelarge, F., de Valicourt, G., Roelkens, G., Van Thourhout, D., Messaoudene, S., Duan, G.H., IEEE Photonics Technol. Lett. 24, 76 (2012)
[3] Maszara, P., Goetz, G., Caviglia, A., McMitterick, J.B., J. Appl. Phys. 64, 4943 (1988)
[4] Fournel, F., Continni, L., Morales, C., Da Fonseca, J., Moriceau, H., Rieutord, F., Barthelemy, A., Radu, I., J. Appl. Phys. 111, 104907 (2012)
[5] Pasquariello, D., Hjort, K., J. Electrochem. Soc. 147, 2343 (2000)
[6] Tong, Q.Y., Gan, Q., Hudson, G., Fountain, G., Enquist, P., Appl. Phys. Lett. 84, 732 (2004)
[7] Liang, D., Chapman, D.C., Li, Y., Oakley, D.C., Napoleone, T., Joudawlkis, P.W., Brubaker, C., Mann, C., Bar, H., Raday, O., Bowers, J.E., Appl. Physics A 103, 213 (2011)
[8] Talneau, A., Roblin, C., Itawi, A., Mauguin, O., Largeau, L., Beaudoin, G., Sagnes, I., Patriarche, G., Appl. Phys. Lett. 102, 212101 (2013)
[9] Pasquariello, D., Camacho, M., Hjort, K., Dosza, L., Szentpali, B., Mat. Sci. Eng. B 80, 164 (2001)
[10] LeBourhis, E., Talneau, A., Sagnes, I., Patriarche, G., Largeau, L., Troadec, D., MRS Proceedings 1510 (2013)
[11] Pantzas, K., Patriarche, G., Bourhis, E. Le, Troadec, D., Itawi, A., Beaudoin, G., Sagnes, I., Talneau, A., Appl. Phys. Lett. 103, 081901 (2013)
[12] Marshall, D.B., Evans, A.G., J. Appl. Phys. 56, 2632 (1948)
[13] Rossington, C., Evans, A.G., Marshall, D.B., Khuri-Yakub, B.T., J. Appl. Phys. 56, 2639 (1948)
[14] Chalker, P.R., Bull, S.J., Rickerby, D.S., Mater. Sci. Eng. A 140, 583 (1991)
[15] Gerberich, W.W., Cordill, M., Rep. Prog. Phys. 69, 2157 (2006)
[16] Bull, S.J., C. R. Mecanique 339, 518 (2011)
[17] Oliver, W.C., Pharr, G.M., J. Mater. Res. 7, 1564 (1992)
[18] Hytch, M., Snoeck, E., Kilaas, R., Ultramicros. 74, 131 (1998)
[19] Kailer, A., Gogotsi, Y.G., Nickel, K.G., J. Appl. Phys. 81, 3057 (1997)
[20] Ge, D.B., Dominich, V., Gogotsi, Y., J. Appl. Phys. 93, 21448 (2003)
[21] Khayyat, M.M., Banini, G.K., Hasko, D.G., Chaudhri, M.M., J. Phys. D 36, 1300 (2003)
[22] Bradby, J.E., Williams, J.S., Swain, M.V., Phys. Rev. B 67, 085205 (2003)
[23] Kramer, D., Huang, H., Kriese, M., Robach, J., Wright, A., Bahr, D., Gerberich, W.W., Acta Mater. 47, 333 (1998)

Instrumented nanoindentation and scanning electron transmission microscopy applied to the study of the adhesion of InP membranes heteroepitaxially bonded to Si

  • Konstantinos Pantzas (a1) (a2), Eric Le Bourhis (a2), Gilles Patriarche (a1), Ahmad Itawi (a1), Grégoire Beaudoin (a1), Isabelle Sagnes (a1) and Anne Talneau (a1)...

Metrics

Full text views

Total number of HTML views: 0
Total number of PDF views: 0 *
Loading metrics...

Abstract views

Total abstract views: 0 *
Loading metrics...

* Views captured on Cambridge Core between <date>. This data will be updated every 24 hours.

Usage data cannot currently be displayed