Thermal analyses of bulk amorphous oxides and silicates of zirconium and hafnium

Published online by Cambridge University Press:  11 February 2011

S. V. Ushakov
Affiliation:
Thermochemistry Facility and NEAT ORU, University of California at Davis, One Shields Avenue, Davis, CA 95616anavrotsky@ucdavis.edu
C. E. Brown
Affiliation:
Thermochemistry Facility and NEAT ORU, University of California at Davis, One Shields Avenue, Davis, CA 95616anavrotsky@ucdavis.edu
A. Navrotsky
Affiliation:
Thermochemistry Facility and NEAT ORU, University of California at Davis, One Shields Avenue, Davis, CA 95616anavrotsky@ucdavis.edu
A. Demkov
Affiliation:
Physical Sciences Research Labs, AZ83/ML26 Motorola, Inc. 7700 S. River Parkway, Tempe, AZ 85284
C. Wang
Affiliation:
Digital DNA Laboratories, Semiconductor Products Sector, Motorola, Inc., 3501 Ed Bluestein Blvd., Austin, TX 78721
B.-Y. Nguyen
Affiliation:
Digital DNA Laboratories, Semiconductor Products Sector, Motorola, Inc., 3501 Ed Bluestein Blvd., Austin, TX 78721
Get access

Abstract

Amorphous pure and Y-doped ZrO2 and HfO2 were prepared by precipitation with ammonia or hydrazine. Amorphous zirconium and hafnium silicates with SiO2 content from 10 to 90 mol % were prepared by sol-gel. Crystallization was studied by differential scanning calorimetry (DSC) at 20 °C/min and crystallite size after crystallization was determined from XRD data. ZrO2 crystallized into the tetragonal phase with ΔH -21 ±2 kJ/mol and HfO2 into the monoclinic phase with ΔH -31 ±2 kJ/mol. Doping with 20 at.% Y decreased crystallite size after crystallization. Crystallization temperatures for pure and Y-doped ZrO2 samples were in the range 420–440 °C. Crystallization temperatures for pure and Y-doped HfO2 samples varied from 470 to 570°C and correlate with surface area. Crystallization onset temperature in silicates increased with silica content from about 650 to 950 °C for ZrO2·SiO2 and from 740 to 1030 °C for HfO2·SiO2. Tetragonal zirconia and hafnia were the only crystalline phases formed below 1100 °C in all zirconium silicates and in hafnium silicates with more than 10 mol% SiO2. Crystallite size after crystallization decreased with increase in silica content. In hafnium silicate, a decrease in HfO2 crystallite size from 5 to 2.5 ±1 nm corresponds to a crystallization enthalpy change from -22 to -15 ±2 kJ/mol. The tetragonal HfO2/amorphous SiO2 interface energy can be calculated from calorimetric data as ∼0.25 J/m2. The critical particle size for the tetragonal to monoclinic transformation of HfO2 in HfO2-SiO2 system is about 6 nm. We predict that tetragonal HfO2 will be stabilized in films thinner than 2 nm.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] JADE, Materials Data Inc, 2002 Google Scholar
[2] Gusev, E., Cabral, C. Jr, Copel, M., Emic, C.D., Gribelyuk, M., Microelectronic Engineering, submitted Google Scholar
[3] Neumayer, D.A., Cartier, E., J. Appl. Phys., 90 (4) 1801–08, (2001)Google Scholar
[4] Maria, J.-P., Wickaksana, D., Parrette, J., Kingon, A.I., J. Mater. Res., Vol. 17, No. 7, (2002)Google Scholar
[5] Garvie, R.G., J. Phys. Chem., 69 (4), 1238–43, (1965)Google Scholar
[6] Wang, , Li, H.P., Stevens, R., J. Mater. Sci. 27(20), 5397–430. (1992)Google Scholar
[7] Zhao, C., Richard, O., Elshocht, S.V., Bender, H., Caymax, M., Vandervorst, W., Gendt, S. D., Heyns, M., Cosnier, V., Chen, J., Roebben, G., Biest, O., Maes, J., Young, E., MRS 2002 Abstracts, N1.5, p. 334, (2002)Google Scholar