Properties of CAT-CVD Silicon Nitride Films and Their Application as Passivation Films

Published online by Cambridge University Press:  10 February 2011

Shinya Okada
Affiliation:
JAIST, (Japan Advanced Institute of Science and Technology), 1-1 Asahidai, Tatsunokuchi, Ishikawa 923-12, Japan
Hideki Matsumura
Affiliation:
JAIST, (Japan Advanced Institute of Science and Technology), 1-1 Asahidai, Tatsunokuchi, Ishikawa 923-12, Japan
Get access

Abstract

Silicon nitride (SiNx) films have been successfully synthesized by the catalytic chemical vapor deposition (cat-CVD) method using a gaseous mixture of silane (SiH4) and ammonia (NH3). In the method, the deposition gases are decomposed by catalytic cracking reactions with a high temperature (1700°C) catalyzer near the substrates, and SiNx films can be deposited at substrate temperatures lower than 400°C without using plasma or photochemical excitation. Nearly stoichiometric Si3N4 films are formed when the flow ratio of NH3 exceeds over 100 times of that of SiH4. These cat-CVD SiNx films show excellent properties. That is, the resistivity, the breakdown voltage, the chemical etch resistance and hydrogen content in the films are almost equivalent to those of high-temperature thermal CVD films. In addition, the surface diffusion length of depositing species is about several-tens μπι and step-coverage itself is conformai. Thus, the cat-CVD SiNx films are regarded not only as a new device passivation films superior to the conventional plasma-CVD films but as a gate insulator for electon devices due to their high quality.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Sinha, A. K., Levinstein, H. J., Smith, T. E., Quintata, G., and Haszko, S. E., J. Electrochem. Soc. 125, 601 (1978).Google Scholar
2 Mito, H. and Sekiguchi, A., J.Vac.Sci. & Tecnol. A4, 475 (1986).Google Scholar
3 Maeda, K. and Umezu, I., J.Appl.Phys. 70, 2745 (1991).Google Scholar
4 Zhang, X., Shi, G., Yang, A., and Shao, D., Thin Solid Films 215, 134 (1992).Google Scholar
5 Parsons, G., Souk, J., and Batey, J., J. Appl.Phys. 70, 1553 (1991).Google Scholar
6 Lanford, W. and Rand, M., J.Appl.Phys. 49, 2473 (1978).Google Scholar
7 Boher, P., Renaud, M., van Ijzendoorn, L.J., and Hily, Y., Appl.Phys.Lett. 54, 511 (1989).Google Scholar
8 Kern, W. and Rosier, R. S., J.Vac.Sci. & Tecnol. 14, 1082 (1977).Google Scholar
9 Matsumura, H., Jpn.J.Appl.Phys. 28, 2157 (1989).Google Scholar
10 Matsumura, H. and Tachibana, H., Appl.Phys.Lett. 47, 833 (1985).Google Scholar
11 Yasui, K., Katoh, H., Komaki, K., and Kaneda, S., Appl.Phys.Lett. 56, 898 (1990).Google Scholar
12 Deshpande, S., Gulari, E., Brown, S., and Rand, S., J.Appl.Phys. 77, 6534 (1995).Google Scholar
13 Dupuie, J., Gulari, E., and Terry, F., J.Electrochem.Soc. 139, 1151 (1992).Google Scholar
14 Horbach, C., Beyer, W., and Wagner, H., J.Non-Cryst. Solids 137&138, 661 (1991).Google Scholar
15 Deshpande, S., Gulari, E., Brown, S., and Rand, S., Mat. Res. Soc. Symp. Proc. 325, 177 (1994).Google Scholar
16 Jeon, Y., Lee, H., and Joo, S., Mat. Res. Soc. Symp. Proc. 284, 9 (1993).Google Scholar