Hostname: page-component-8448b6f56d-sxzjt Total loading time: 0 Render date: 2024-04-23T17:36:20.332Z Has data issue: false hasContentIssue false

Physical, Electrical, and Piezoelectric Properties of Hot-Forged Sr2(NbTa)2O7 Ceramics

Published online by Cambridge University Press:  15 February 2011

Paul A. Fuierer
Affiliation:
Materials Research Laboratory, The Pennsylvania State Universtiy, University Park, PA 16802
Tom R. Shrout
Affiliation:
Materials Research Laboratory, The Pennsylvania State Universtiy, University Park, PA 16802
Robert E. Newnham
Affiliation:
Materials Research Laboratory, The Pennsylvania State Universtiy, University Park, PA 16802
Get access

Abstract

Solid solution compositions of Sr2(NbxTa1−x)2O7 ceramics with Tr ranging from 450°C to 1342°C were fabricated utilizing a hot-forging technique to achieve preffered grain orientation and thus enhance poling. Translucent samples with greater than 99% theoretical density were obtained using this process. Depending on composition, the degree of orientation as determined by x-ray diffraction was found to be 75% to 95%. The thermal expansion, resistivity, and dielectric constant were shown to be very anisotropic. The direction perpendicular to the forging axis proved to be the ferroelectric “easy” direction, exhibiting hysteresis behavior. Piezoactivity in PLS polycrystals was measured for the first time. Hot-forged samples were electrically poled and the electromechanical properties determined using the five different modes of vibration. For Sr2(Nb0.5Ta0.5)2O7: N24=1504 Hz-m, s44=18.2×10-12m2/N, k24=3.0%, d24=2.6 pC/N, g24=6.3×10-3 Vm/N, and Qm=1100. This material was also shown to resist depoling when exposed to temperatures as high as 650°C.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Ishizawa, N., Marumo, F., Kawamura, T. and Kimura, M., Acta Cryst. D 331, 1912 (1975).Google Scholar
2. Ishizawa, N., Marumo, F. and Iwai, S., Acta Cryst. B37, 26 (1981).Google Scholar
3. Nanamatsu, S., Kimura, M. and Kawamura, T., J. Phys. Soc. Japan 38 (3), 81 (1975).Google Scholar
4. Akishige, Y., Yoneya, Y., Ohi, K. and Sawaguchi, E., J. Phys. Soc. Japan 5 398 (1989).Google Scholar
5. Nanamatsu, S., Kimura, M., Doi, K. and Takahashi, M.,” J. Phys. Soc. Japan 30, 300 (1971).Google Scholar
6. Nanamatsu, S. and Kimura, M., J. Phys. Soc. Japan 36, 1495 (1974).CrossRefGoogle Scholar
7. Nanamatsu, S., Kimura, M., Doi, K., Matsushita, S. and Yamada, N., Ferroelectrics 8, 511(1974)CrossRefGoogle Scholar
8. Takenaka, T. and Sakata, K., Japan. J. Appl. Phys. 12 (1), 31 (1980).CrossRefGoogle Scholar
9. Fuierer, P.A. and Newnham, R.E., J. Am. Ceram. Soc. 24 (11), 2876 (1991).Google Scholar
10. Sych, A.M., Titov, Y.A. and Nedil'ko, S.A., Zhurnal Neorg. Khimii 25, 2056 (1980) [Russain J. Inorg. Chem. 25 (8), 1139 (1980)].Google Scholar
11. Ohi, K. and Kojima, S., Japan. J. Appl. Phys. Supplement 24–2, 817 (1985).Google Scholar
12. Lotgering, F.K., J. Inorg. Nucl. Chem. 2, 113 (1959).CrossRefGoogle Scholar
13. IEEE Standard on Piezoelectricity, ANSI/IEEE Std 176-1978, IEEE, New York (1978).Google Scholar
14. Akishige, Y., Kobayashi, M., Ohi, K. and Sawaguchi, E., J. Phys Soc. Japan 55 (7), 2270 (1986)Google Scholar