Humidity and temperature control accessories for Hysitron Triboscope have been developed to study the environmental influence on in situ properties of drying coatings. Mechanical properties of drying poly (vinyl alcohol) (PVOH) and poly (vinyl pyrrolidone) (PVP) coatings on silicon wafer were measured under different humidities. The modulus results were compared with outputs of elastic, plastic and viscoelastic theories of indentation testing.

Copyright

References

Hide All
1. Gutoff, E. B. and Cohen, E. D., Coating and Drying Defects: Troubleshooting Operating Problems, (J. Wiley and Sons, New York, 1995).
2. Errede, L. A., Heinrich, P. J. and Tiers, G. V. D., J. Appl. Polym. Sci., 54, 669 (1994).
3. Crapiste, G. H., Whitaker, S. and Rotstein, E., Chem. Eng. Sci., 43, 2929 (1988).
4. Cairncross, R. A., Jeyadev, S., Dunham, R. F., Evans, K., Francis, L. F. and Scriven, L. E., J. Appl. Polym. Sci., 58, 1279 (1995).
5. Errede, L. A., J. Polym. Sci., Polym. Chem., 28, 857 (1990).
6. Finch, C. A., Polyvinyl Alcohol-Develop, (Wiley, New York, 1992).
7. Oliver, W. C. and Pharr, G. M., J. Mater. Res., 7, 1564 (1992).
8. Sneddon, I. N., Int. J. Eng. Sci. 3, 47 (1965).
9. Gerberich, W. W., Yu, W., Kramer, D., Strojny, A., Bahr, D., Lilleodden, E. and Nelson, J., J. Mater. Res., 13, 421 (1998).
10. Cheng, L., Scriven, L. E. and Gerberich, W. W., in Proceeding of the 4th World Congress on Computational Mechanics, (Buenos Aires, Argentina, 1998).
11. Cheng, L., Xia, X., Yu, W., Scriven, L. E. and Gerberich, W. W., J. Polym. Sci.: Part B: Polym. Phys., 37 (1999).
12. Cheng, L., Scriven, L. E. and Gerberich, W. W., in Fundamentals of Nanoindentation and Nanotribology, edited by Moody, N.R., Gerberich, W.W., Burnham, N. and Baker, S. P. (Mater. Res. Soc. Proc. 522, Warrendal, PA 1998), 193.
13. Cheng, L., private communication.
14. Dibbern-Brunelli, D., Atvars, T. D., Joekes, I. and Barbosa, V. C., J. Appl. Polym. Sci., 69, 645 (1998).
15. Tadokoro, S. Seki and Nitta, I., Bull. Chem. Soc. Jpn., 28, 559 (1955).

Nanoindentation Probing of Environmental Effects on Polymer Coating Properties

  • X. Xia (a1), D. Rowenhorst (a1), K. B. Yoder (a1), L. E. Scriven (a1) and W. W. Gerberich (a1)...

Metrics

Full text views

Total number of HTML views: 0
Total number of PDF views: 0 *
Loading metrics...

Abstract views

Total abstract views: 0 *
Loading metrics...

* Views captured on Cambridge Core between <date>. This data will be updated every 24 hours.

Usage data cannot currently be displayed