Low Energy Atom Scattering Spectroscopy for Insulator Surface Analysis: MgO(111) Surfaces

  • K. Umezawa (a1)

Abstract

This study described a low-energy atom scattering system combined with a time-of-flight spectrometer and an ultra high vacuum chamber for insulator surface structural analysis. We show one of examples to study of MgO(111) surface analysis. A visual image of Mg atoms due to the projected blocking pattern represents the crystalline structure of the MgO(111) surfaces. This figure shows the trajectory of scattered 4He0 particles due to Mg atoms along low-index lattice planes and crystallographic directions. Insulator surface structural analysis becomes more important in materials sciences.

Copyright

References

Hide All
Feldman, L. C, Mayer, J. W., Fundamentals of Surface and Thin Film Analysis, (North-Holland, 1986).
Umezawa, K., Nakanishi, S., Hayashi, H., Higashitsutsumi, H., Nagasawa, H., Ogai, K., MRS online proceeding library, 2011, vol. 1318, mrsf10-1318-ss05-05.
Smith, D. P., J. Appl. Phys. 38, 340 (1967).
Katayama, M., Nomura, E., Kanekuma, N., Soejima, H., Aono, M., Nucl. Instr. Meth. B 33, 857 (1988).
Sumitomo, K., Oura, K., Katayama, I., Shoji, F., Hanawa, T., Nucl. Instrum. Meth. B 33, 871 (1988).
Yoshimoto, M., Maeda, T.,Shimozono, K., Koinuma, H., Shinohara, M., Ishiyama, O. and Ohtani, F., Appl. Phys. Lett. 65, 3197 (1994).
Umezawa, K., Nakanishi, S., Kojima, K., Yoshimura, M., Ueda, K., Gibson, W. M., Phys. Rev. B 63, 035402 (2001).
Rabalis, J. W., Low Energy Ion Surface Interactions, (Wiley, 1994).
Moliére, G., Naturforsch, Z.. Teil A 2 (1947) 133.
Firsov, O. B., Sov. Phys, JETP 6 (1958) 534.

Keywords

Low Energy Atom Scattering Spectroscopy for Insulator Surface Analysis: MgO(111) Surfaces

  • K. Umezawa (a1)

Metrics

Full text views

Total number of HTML views: 0
Total number of PDF views: 0 *
Loading metrics...

Abstract views

Total abstract views: 0 *
Loading metrics...

* Views captured on Cambridge Core between <date>. This data will be updated every 24 hours.

Usage data cannot currently be displayed.