Fiber-Reinforced Tubular Composites by Chemical Vapor Infiltration°

Published online by Cambridge University Press:  15 February 2011

D. P. Stinton
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee 37831
R. A. Lowden
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee 37831
T. M. Besmann
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee 37831
Get access

Abstract

A forced-flow thermal-gradient chemical vapor infiltration process has been developed to fabricate composites of thick-walled tubular geometry common to many components. Fibrous preforms of different fiber architectures (3-dimensionally braided and filament wound) have been investigated to accommodate components with different mechanical property requirements. This paper will discuss the fabrication of tubular, fiber-reinforced SiC matrix composites and their mechanical properties.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Simon, G. and Bunsell, A. R., “Creep Behavior and Structural Characterization at High Temperatures of Nicalon SiC Fibers,” J. Mater. Sci. 19, 3658 (1984).Google Scholar
2. Lamicq, P. J., Bernhart, G. A., Dauchier, M. M., and Mace, J. G., “SiC/SiC Composite Ceramics,” Am. Ceram. Soc. Bull. 65 (no. 2), 336 (1986).Google Scholar
3. Hurwitz, F. I., Heimann, P. J., Gyekenyesi, J. Z., Masnovi, J., and Bu, X. Ya, “Polymeric Routes to Silicon Carbide and Silicon Oxycarbide CMC,” Cer. Eng. Sci. Proc., 12(7–8), 1292 (1991).Google Scholar
4. Boisvert, R. P., and Diefendorf, R. J., “Polymeric Precursor SiC Matrix Composites,” Cer. Eng. Sci. Proc. 9(7–8), 873 (1988).Google Scholar
5. Lundberg, R., and Goursat, P., “Silicon Carbo-Nitride Ceramic Matrix Composites by Polymer Pyrolysis,” Developments in the Science and Technology of Composite Materials, ed. Bunsell, A. R., Lamicq, P., and Massiah, A., Elsevier Applied Science, London, p. 93, (1989).Google Scholar
6. Lightfoot, A., Ewart, L., Haggerty, J., Cai, Z. O., Ritter, J., and Nair, S., “Processing and Properties of SiC Whisker- and Particulate-Reinforced Reaction Bonded Si3N4 ,” Cer. Eng. Sci. Proc. 12(7–8), 1265 (1991).Google Scholar
7. Starr, T. L., Harris, J. N., Freeman, G. B., and Mohr, D. L., “Reaction Sintered Silicon Nitride Composites with Continuous Fiber Reinforcement,” Proceedings of the Fifth Annual Conference on Fossil Energy Materials, ORNL Report CONF-9105184, 47 (1991).Google Scholar
8. Christin, F., Heraud, L, Choury, J. J., Naslain, R., and Hagemuller, P., “In-Depth Chemical Vapor Deposition of SiC within Porous Carbon-Carbon Materials,” Proc. 3rd Eur. Conf. on Chem. Vapor Dep., 154 (1980).Google Scholar
9. Warren, J. W., “Fiber- and Grain-Reinforced CVI Silicon Carbide Matrix Composites,” Cer. Eng. Sci. Proc. 6(7–8), 64 (1985).Google Scholar
10. Fisher, R. E., Burkland, C. V., and Bustamante, W. E., “Ceramic Composites Based on Chemical Vapor Infiltration,” Proc. of the Metal and Ceramic Matrix Composite Processing Conf., Battelle Columbus Labs., Columbus, Ohio, Nov. 14, 1984.Google Scholar
11. Headinger, M. H., and Purdy, M. J., “Design of a Production-Scale Process for Coating Composite Structures,” Surface and Coat. Tech., 33, 433 (1987).Google Scholar
12. Stinton, D. P., Caputo, A. J., and Lowden, R. A., “Synthesis of Fiber-Reinforced SiC Composites by Chemical Vapor Infiltration,” Am. Ceram. Soc. Bull., 65[2], 347–50 (1986).Google Scholar
13. Caputo, A. J., and Lackey, W. J., “Fabrication of Fiber-Reinforced Ceramic Composites by Chemical Vapor Infiltration,” Cer. Eng. Sci. Proc., 5(7–8), 654–67 (1984).Google Scholar
14. Besmann, T.M., Sheldon, B. W., Lowden, R. A., and Stinton, D. P., “Vapor-Phase Frication and Properties of Continuous-Filament Ceramic Composites,” Science, Vol.253, 1104–9 (1991).Google Scholar
15. Stinton, D. P., Besmann, T. M., and Lowden, R. A., “Advanced Ceramics by Chemical Vapor Deposition Techniques,” Am. Ceram. Soc. Bull. 67(2), 350–55 (1988).Google Scholar
16. Yajima, S., et al., “Synthesis of Continuous SiC Fibers with High Tensile Strength, “J. Am. Ceram. Soc., 59(7–8), 2427 (1976).CrossRefGoogle Scholar
17. Yajima, S., et al., “Anomalous Characteristics of the Microcrystalline State of SiC Fibers,” Nature 27(21), 706–7 (1979).Google Scholar
18. Lowden, R. A., Stinton, D. P., and Besmann, T. M., “Characterization of Fiber-Matrix Interfaces in Ceramic Composites,” Conference Proceedings, Whisker- and Fiber-Toughened Ceramics, ASM International, 253–64, 1988.Google Scholar
19. Stinton, D. P., Lowden, R. A., and Krabill, R. H., “Mechanical Property Characterization of Fiber-Reinforced SiC Matrix Composites,” ORNL Report No. ORNL/TM-11524, April 1990.Google Scholar