Development of Environmental Cell and its Application to Hydrogen Storage Materials

Published online by Cambridge University Press:  26 February 2011

Koya Okudera
Affiliation:
okudera@eng.hokudai.ac.jp, Hokkaido University, Graduate School of Engineering, N-13, W-8, Kita-ku, Sapporo, 0608628, Japan
Koichi Hamada
Affiliation:
hamada@nano.ist.hokudai.ac.jp, Graduate School of Engineering, Hokkaido University, Division of Materials Science and Engineering, Sapporo, Hokkaido, 060-8628, Japan
Takanori Suda
Affiliation:
suda@eng.hokudai.ac.jp, Graduate School of Engineering, Hokkaido University, Division of Materials Science and Engineering, Sapporo, Hokkaido, 060-8628, Japan
Naoyuki Hashimoto
Affiliation:
hasimoto@eng.hokudai.ac.jp, Graduate School of Engineering, Hokkaido University, Division of Materials Science and Engineering, Sapporo, Hokkaido, 060-8628, Japan
Somei Ohnuki
Affiliation:
ohnuki@eng.hokudai.ac.jp, Graduate School of Engineering, Hokkaido University, Division of Materials Science and Engineering, Sapporo, Hokkaido, 060-8628, Japan
Yasuaki Kawai
Affiliation:
e0423@mosk.tytlabs.co.jp, Toyota Central R&D Labs. Inc., Nagakute, Aichi, 480-1192, Japan
Yoshitsugu Kojima
Affiliation:
kojimay@hiroshima-u.ac.jp, Hiroshima University, Institute for Advanced Materials Research, Higashi-Hiroshima, Hiroshima, 739-8530, Japan
Get access

Abstract

High-resolution and “environmental cell” microscopy were applied for surveying the reaction of hydrides in Vanadium and Magnesium based alloys, which are candidate for hydrogen storage materials of advanced hydrogen energy systems. For clarify the hydrogenation process, in-situ experiment was carried out by using 200 kV TEM equipped with a newly developed environmental cell, which is enable to observe transmitted image and electron-diffraction under gas reaction under hydrogen environment of 0.1 MPa at room temperature. In case of Vanadium, bending fringe was created under hydrogen-gas of 0.1 MPa, which means that hydrogen reaction is not so quick in this case, and the local stress due to the hydrogen solution caused the fringes. In case of Magnesium, the gas reacted with the powders and showed the swelling, where the surface steps with several ten nm become to more straight, and also SADP showed the formation of MgH2. In-situ experiment for hydrogenation reaction by using the environmental cell has started recently, therefore the precise studies will be continued, as well as its improvement, especially in the transparence films.

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Yamamoto, T., Inui, H. and Yamaguchi, M., Mater. Sci. Eng. A, 329–331 367371 (2002)Google Scholar
2. Nakagawa, T., Ichikawa, T., Iida, R., Leng, H., Takeichi, N., Kiyobayashi, T., Takeshita, H. and Fujii, H., J. Alloys Comp., 430 217221 (2007)Google Scholar
3. Marikar, P., Brodsky, M. B., Sowers, C. H., Zaluzec, N. J., Ultramicroscopy, 29 247256 (1989)Google Scholar
4. Gai, P. L., J. Solid State Chem., 49 2542 (1983)Google Scholar
5. Raynerd, G., Venables, J. A., 23 432433 (1987)Google Scholar
6. Robertson, I. M., Engineering Fracture Mechanics, 68 671692 (2001)Google Scholar
7. Akimoto, T., Hirohata, Y., Shimada, M., Sugi, H., Proceedings of the 57th Annual Meeting of the Japanese Society of Electron Microscopy, 119 (2001)Google Scholar
8. Fujita, K., Huang, Y. C., Tada, M., J. Japan Inst. Metals, 43 601609 (1979)Google Scholar