Comparison of Different Fluorine-treatments for Improved High Temperature Oxidation Resistance of TiAl-alloys

Published online by Cambridge University Press:  07 March 2011

A. Donchev
Affiliation:
DECHEMA e.V. Karl-Winnacker-Institut, Theodor-Heuss-Allee 25; D-60486 Frankfurt/Main, Germany
M. Schütze
Affiliation:
DECHEMA e.V. Karl-Winnacker-Institut, Theodor-Heuss-Allee 25; D-60486 Frankfurt/Main, Germany
A. Kolitsch
Affiliation:
Forschungszentrum Dresden-Rossendorf e.V. Institute of Ion Beam Physics and Materials Research, Bautzener Landstraße 128, D-01328 Dresden, Germany
R. Yankov
Affiliation:
Forschungszentrum Dresden-Rossendorf e.V. Institute of Ion Beam Physics and Materials Research, Bautzener Landstraße 128, D-01328 Dresden, Germany
Get access

Abstract

Intermetallic TiAl-alloys can replace the heavier Ni-based superalloys in several high temperature applications with regards to their mechanical properties, however they can not be used at temperatures above 800°C in oxidizing environments for longer times because of insufficient oxidation resistance. Despite an Al-content of about 45 at.% in technical alloys, no protective alumina layer is formed because the thermodynamic stabilities of titanium oxide and aluminum oxide are of the same order of magnitude. Therefore a mixed TiO2/Al2O3-scale is formed which is fast growing so that the metal consumption rate is quite high. On the other hand the formation of a slow growing alumina layer is promoted by a fluorine treatment. This so called fluorine effect leads to the preferential intermediate formation of gaseous aluminum fluorides at elevated temperatures if the fluorine content at the surface stays within a defined concentration range. These fluorides are converted into solid Al2O3 due to the high oxygen partial pressure of the high temperature service environment forming a protective pure Al2O3 surface scale. In this paper results of high temperature oxidations tests of several technical TiAl-alloys will be presented. Different F-treatments e.g. dipping or spaying which are easy to apply have been used and their results will be compared. The mass change data of the F-treated specimens are always lower than those of the untreated ones. Post experimental investigations such as light microscopy, scanning electron microscopy and energy dispersive X-ray analysis reveal the formation of a thin alumina layer on the F-treated samples after optimization of the process while a thick mixed scale is found on the untreated samples. The results will be discussed in view of an optimized procedure and the future use of TiAl-components in high temperature environments.

Type
Research Article
Copyright
Copyright © Materials Research Society 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Taniguchi, S., Materials and Corrosion 48 1 (1997)Google Scholar
2. Schütze, M., Hald, M., Materials Science Engineering A 239–240 847 (1997)Google Scholar
3. Donchev, A., Zschau, H.-E., Schütze, M., Materials at High Temperatures 22 309 (2005)Google Scholar
4. Donchev, A., Richter, E., Schütze, M., Yankov, R., J. Alloys and Compounds 452 7 (2008)Google Scholar
5. Rahmel, A., Quadakkers, W.J., Schütze, M., Materials and Corrosion 46 271 (1995)Google Scholar
6. Donchev, A., Gleeson, B., Schütze, M., Intermetallics 11 387 (2003)Google Scholar
7. Masset, P.J., Yankov, R., Kolitsch, A., Schütze, M., Materials Science Forum 638–642 1374 (2010)Google Scholar
8. Sorell, G., Materials at High Temperatures 14 207 (1997)Google Scholar
9. Zschau, H.-E., Schütze, M., Materials and Corrosion 59 619 (2008)Google Scholar
10. Donchev, A., Richter, E., Schütze, M., Yankov, R., Intermetallics 14 1168 (2006)Google Scholar
11. Donchev, A., Schütze, M., Materials Science Forum 638–642 1294 (2010)Google Scholar
12. Schütze, M., “Protective Oxide Scales and their Breakdown”, ed. Holmes, D.R. (John Wiley & Sons 1997) p. 67114 Google Scholar
13. Rakowski, J.M., Pettit, F.S., Meier, G.H., Dettenwanger, F., Schumann, E., Rühle, M., Scripta Metallurgica et Materialia 33 997 (1995)Google Scholar