Chemical Structure of Native Oxide Grown on Hydrogenterminated Silicon Surfaces

Published online by Cambridge University Press:  25 February 2011

M. Takakura
Affiliation:
Department of Electrical Engineering, Hiroshima UniversityHigashi-Hiroshima 724, Japan
T. Yasaka
Affiliation:
Department of Electrical Engineering, Hiroshima UniversityHigashi-Hiroshima 724, Japan
S. Miyazaki
Affiliation:
Department of Electrical Engineering, Hiroshima UniversityHigashi-Hiroshima 724, Japan
M. Hirose
Affiliation:
Department of Electrical Engineering, Hiroshima UniversityHigashi-Hiroshima 724, Japan
Get access

Abstract

Chemical bonding features and suboxide compositions in native oxide grown on chemically-cleaned hydrogen-terminated Si(100) surfaces stored in pure water have been studied by using surface sensitive infrared spectroscopy and x-ray photoelectron spectroscopy. The LO phonon peak for the native oxide is located at 1210cm−1, which is shifted to a significantly lower wavenumber side than the ultrathin thermal oxide peak at 1250cm−1. This is because an appreciable amount of SiHx bonds are incorporated in the native oxide/Si interface and such hydrogen termination in the network dramatically reduces strained bonds in the interface. Very weak Si2+ suboxide signal from the oxide grown in pure water is also explained by the incorporated SiHx bonds which interrupt the Si2+ suboxide formation in the interface.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Takahagi, T., Nagai, I., Ishitani, A., Kuroda, H. and Nagasawa, Y, J. Appl. Phys. 64 3516 (1988).CrossRefGoogle Scholar
[2] Gould, G. and Irene, E. A., J. Electrochem. Soc 134 1031 (1987).CrossRefGoogle Scholar
[3] Sugiyama, K., Igarashi, T., Moriki, K., Nagasawa, Y., Aoyama, T., Sugino, R., Ito, T. and Hattori, T., Jpn. J. Appl. Phys. 29 L2401 (1990).CrossRefGoogle Scholar
[4] Sunada, T., Yasaka, T., Takakura, M., Sugiyama, T., Miyazaki, S., and Hirose, M., Jpn. J. Appl. Phys. 29 L2408 (1990).CrossRefGoogle Scholar
[5] Chabal, Y. J., Surf. Sci. Reports 8 211 (1988).CrossRefGoogle Scholar
[6] Raider, S. I. and Flitsch, R., IBM J. Res. Develop. 22 294 (1978).CrossRefGoogle Scholar
[7] Himpsel, F. J., McFeely, F. R., Taleb-Irrahimi, A., Yarmoff, A. and Hollinger, G., Phys. Rev. B 38 6084 (1988).CrossRefGoogle Scholar
[8] Lucovsky, G., Solid State Commun. 29 571 (1979).CrossRefGoogle Scholar
[9] Takahagi, T., Ishitani, A., Kuroda, H. and Nagasawa, Y., J. Appl. Phys. 68 2187 (1990).CrossRefGoogle Scholar