Aluminum-Matrix Aluminum Nitride Particle Composite as a Low-Thermal-Expansion Thermal Conductor

Published online by Cambridge University Press:  15 February 2011

Shy-Wen Lai
Affiliation:
Composite Materials Research Laboratory, State University of New York at Buffalo, Buffalo, NY 14260–4400
D. D. L. Chung
Affiliation:
Composite Materials Research Laboratory, State University of New York at Buffalo, Buffalo, NY 14260–4400
Get access

Abstract

Aluminum-matrix composites containing AIN or SiC particles were fabricated by vacuum infiltration of liquid aluminum into a porous particulate preform under an argon pressure of up to 41 MPa. Al/AIN was superior to Al/SiC in thermal conductivity. At 59 vol.% AIN, Al/AlN had a thermal conductivity of 157 W/m. °C and a thermal expansion coefficient of 9.8 × 10−-6°C−1 (35–100 °C). Al/AlN had similar tensile strength and higher ductility compared to Al/SiC of a similar reinforcement volume fraction at room temperature, but exhibited higher tensile strength and higher ductility at 300–400°C. The ductility of Al/AlN increased with increasing temperature from 22 to 400°C, while that of Al/SiC did not change with temperature. The superior high temperature resistance of Al/AlN is attributed to the lack of a reaction between Al and AIN, in contrast to the reaction between Al and SiC in AI/SiC.

Type
Research Article
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Geiger, Alan L. and Jackson, Michael, Adv. Mat. Proc. 136(1), 23 (1989).Google Scholar
2. Alan Geiger, L., private communications.Google Scholar
3. Aghajanian, M.K., Burke, J.T., White, D.R. and Nagelburg, A.S., SAMPE Q. 20(4), 43 (1989).Google Scholar
4. Toy, C. and Scott, W.D., J. Am. Ceram. Soc. 73(1), 97101 (1990).Google Scholar
5. Chiou, Jeng-Maw and Chung, D.D.L., J. Mater. Sci. 28, 14351446 (1993); Jeng-Maw Chiou and D.D.L. Chung, J. Mater. Sci., 28, 1447–1470 (1993); Jeng-Maw Chiou and D.D.L. Chung, J. Mater. Sci., 28, 1471–1487 (1993).CrossRefGoogle Scholar