Mapping of the Initial Volume at the Onset of Plasticity in Nanoindentation

Published online by Cambridge University Press:  01 February 2011

Tingting Zhu
Affiliation:
t.zhu@qmul.ac.uk, Queen Mary University of London, Materials, Mile End Street, London, E1 4NS, United Kingdom, 02078827418
K.M.Y. P'ng
Affiliation:
m.y.png@qmul.ac.uk, Queen Mary University of London, Centre for Materials Research, London, E1 4NS, United Kingdom
M. Hopkinson
Affiliation:
m.hopkinson@sheffield.ac.uk, University of Sheffield, Department of Electronic and Electric Engineering, Sheffield, S1 3JD, United Kingdom
A.J. Bushby
Affiliation:
a.j.bushby@qmul.ac.uk, Queen Mary University of London, Centre for Materials Research, London, E1 4NS, United Kingdom
D.J. Dunstan
Affiliation:
d.j.dunstan@qmul.ac.uk, Queen Mary University of London, Centre for Materials Research, London, E1 4NS, United Kingdom
Get access

Abstract

Understanding the finite volume throughout which plastic deformation begins is necessary to understand the mechanics of small-scale deformation. In indentation using spherical indenters, conventional yield criteria predict that yield starts at a point on the axis and at a depth of half the contact radius. However, Jayaweera et al (Proc. Roy. Soc. 2003)[4] concluded that yield occurs over a finite volume at least 100 nm thick. Semiconductor superlattice structures, in which the stress and thickness of individual layers can be varied and in which known internal stresses can be incorporated, open up new possibilities for investigation that cannot be achieved by varying external stresses on a homogenous specimen. We have designed samples with bands of highly strained InGaAs superlattice, which are essentially bands of low yield-stress material devoid of other metallurgical artifacts. These bands are placed at different depths in a series of samples. Spherical indenters with a range of radii were used to determine the elastic-plastic transition. The stress field from different sized indenters interacts with the low yield-stress material at different depths below the surface to map out the size of the initial yield volume.

Type
Research Article
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below.

References

1 Minori, A. M., Asif, S. A. Syed, Shan, Z., Stach, E.A., Cyrankowshi, E., Wyrobek, T.J. and Warren, O. L., Nature Materials Letters, 5 697 (2006).CrossRefGoogle Scholar
2 Kiely, J.D., Jarausch, K.F., Houston, J.E., Russell, P.E., Journal of Materials Research, 14 2219 (1999)CrossRefGoogle Scholar
3 P'ng, K.M.Y., Bushby, A.J. and Dunstan, D.J., Mat. Res. Soc. Symp. Proc. 778 U6.3.1 (2003)Google Scholar
4 Jayaweera, N. B., Downes, J. R., Frogley, M. D., Hopkinson, M., Bushby, A.J., Kidd, P., Kelly, A. and Dunstan, D.J., Proc. Roy. Soc. A., 459 2049 (2003)CrossRefGoogle Scholar
5 Jayaweera, N.B., Downes, J.R., Dunstan, D.J., Bushby, A.J., Kidd, P. and Kelly, A., MRS Symp. Proc. 634 B4.10 (2001)Google Scholar
6 Brenchley, M.E., Hopkinson, M., Kelly, A. and Dunstan, D.J., Phys. Rev. Letters 78 3912 (1997)CrossRefGoogle Scholar
7 Field, J.S. and Swain, M.V. J. Mater. Res. 8 297 (1993)CrossRefGoogle Scholar
8 Zhu, T.T., Bushby, A.J. and Dunstan, D.J., Journal of Mech. Physics Solids in press.Google Scholar
9 Zhu, T.T., Hou, X., Bushby, A.J. and Dunstan, D.J., Journal of Physics D in press.Google Scholar
10 Lloyd, S. J., P'ng, K. M.Y., Bushby, A.J., Dunstan, D.J. and Clegg, W. J. Philosophical Magazine,85 2469 (2005)CrossRefGoogle Scholar

Full text views

Full text views reflects PDF downloads, PDFs sent to Google Drive, Dropbox and Kindle and HTML full text views.

Total number of HTML views: 0
Total number of PDF views: 10 *
View data table for this chart

* Views captured on Cambridge Core between September 2016 - 18th January 2021. This data will be updated every 24 hours.

Hostname: page-component-77fc7d77f9-fgqm6 Total loading time: 0.802 Render date: 2021-01-18T21:23:21.296Z Query parameters: { "hasAccess": "0", "openAccess": "0", "isLogged": "0", "lang": "en" } Feature Flags last update: Mon Jan 18 2021 20:56:51 GMT+0000 (Coordinated Universal Time) Feature Flags: { "metrics": true, "metricsAbstractViews": false, "peerReview": true, "crossMark": true, "comments": true, "relatedCommentaries": true, "subject": true, "clr": true, "languageSwitch": true, "figures": false, "newCiteModal": false, "shouldUseShareProductTool": true, "shouldUseHypothesis": true, "isUnsiloEnabled": true }

Send article to Kindle

To send this article to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about sending to your Kindle. Find out more about sending to your Kindle.

Note you can select to send to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be sent to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Mapping of the Initial Volume at the Onset of Plasticity in Nanoindentation
Available formats
×

Send article to Dropbox

To send this article to your Dropbox account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Dropbox.

Mapping of the Initial Volume at the Onset of Plasticity in Nanoindentation
Available formats
×

Send article to Google Drive

To send this article to your Google Drive account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Google Drive.

Mapping of the Initial Volume at the Onset of Plasticity in Nanoindentation
Available formats
×
×

Reply to: Submit a response


Your details


Conflicting interests

Do you have any conflicting interests? *