Hostname: page-component-559fc8cf4f-lzpzj Total loading time: 1.793 Render date: 2021-03-08T04:33:20.732Z Has data issue: true Feature Flags: { "shouldUseShareProductTool": true, "shouldUseHypothesis": true, "isUnsiloEnabled": true, "metricsAbstractViews": false, "figures": false, "newCiteModal": false, "newCitedByModal": true }

Inter Laboratory Comparison and Analysis on Mechanical Properties by Nanoindentation

Published online by Cambridge University Press:  01 February 2011

J. M. Alvarado-Orozco
Affiliation:
Centro de Investigación y de Estudios Avanzados del IPN, Unidad Querétaro, Libramiento Norponiente 2000, Real de Juriquilla, 76230, Querétaro, México.
C. Cárdenas-Jaramillo
Affiliation:
Centro de Investigación y de Estudios Avanzados del IPN, Unidad Querétaro, Libramiento Norponiente 2000, Real de Juriquilla, 76230, Querétaro, México.
D. Torres-Torres
Affiliation:
Centro de Investigación y de Estudios Avanzados del IPN, Unidad Querétaro, Libramiento Norponiente 2000, Real de Juriquilla, 76230, Querétaro, México.
R. Herrera-Basurto
Affiliation:
CENAM-Dirección de Metrología de Materiales, 76241, Querétaro, México.
A. Hurtado-Macias
Affiliation:
Centro de Investigación en Materiales Avanzados, S.C, Laboratorio Nacional de Nanotecnología, Miguel de Cervantes 120, Complejo Industrial Chihuahua, 31109, Chihuahua, México.
J. Muñoz-Saldaña
Affiliation:
Centro de Investigación y de Estudios Avanzados del IPN, Unidad Querétaro, Libramiento Norponiente 2000, Real de Juriquilla, 76230, Querétaro, México. Centro de Investigación en Materiales Avanzados, S.C, Laboratorio Nacional de Nanotecnología, Miguel de Cervantes 120, Complejo Industrial Chihuahua, 31109, Chihuahua, México.
G. Trápaga-Martinez
Affiliation:
Centro de Investigación y de Estudios Avanzados del IPN, Unidad Querétaro, Libramiento Norponiente 2000, Real de Juriquilla, 76230, Querétaro, México.
Get access

Abstract

This contribution presents the results obtained by a Mexican laboratory in the Asia-Pacific Economy Cooperation Interlaboratory Comparison (IC) on mechanical properties by nanoindentation from 2008 using fused silica and polycarbonate as samples. Reduced modulus and indentation hardness are the parameters asked to be measured and compared. The aim for this paper is to show and to discuss the so called “indentation size effect” (ISE) on the indentation hardness of fused silica. Using the spherical formulation of the ISE model for crystalline materials, the macroscopic hardness and material length scale of fused silica are determined as (7.34 ± 0.085) GPa and (166.36 ± 14) nm, respectively.

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below.

References

[1] Oliver, W.C. and Pharr, G.M., J. Mater. Res., 7, 15641583, (1992).CrossRefGoogle Scholar
[2] 2008 APEC ISTWG Project Interlaboratory Comparison on Mechanical Properties by Nano Indentation - Measurement Report Draft 1. (2008).Google Scholar
[3] Fischer-Cripps, A.C., Nanoindentation, 249, Berlin: Springer (2004).CrossRefGoogle Scholar
[4] Hurtado-Macias, A., Muñoz-Saldaña, J., Espinoza-Beltran, F.J., Scholz, T., Swain, M.V. and Schneider, G.A., J. Phys. D: Appl. Phys. 41, 035407, (2008).CrossRefGoogle Scholar
[5] Nix, W.D. and Gao, H. J. Mech. Phys. Solids, 46, 411–25, (1998).CrossRefGoogle Scholar
[6] Zhu, T.T., Hou, X.D., Bushby, A.J. and Dunstan, D.J., J. Phys. D: Appl. Phys., 41, 074004, 6, (2008).CrossRefGoogle Scholar
[7] Scholz, T., Muñoz-Saldaña, J., Schneider, G.A. and Swain, M.V., Appl. Phys. Lett., 84 (16), 30553057, (2004).CrossRefGoogle Scholar
[8] Fleck, N.A, Muller, G.M., Ashby, M.F. and Hutchinson, J.W., Acta Metall. et Mater., 42 (2), 475487, (1994).CrossRefGoogle Scholar
[9] Ma, Q. and Clarke, D.R., J. of Materials Research, 10 (4) 853863, (1995).CrossRefGoogle Scholar
[10] Swadener, J.G., George, E.P. and Pharr, G.M., J. Mech. Phys. Solids, 50, 681694, (2002).CrossRefGoogle Scholar

Full text views

Full text views reflects PDF downloads, PDFs sent to Google Drive, Dropbox and Kindle and HTML full text views.

Total number of HTML views: 0
Total number of PDF views: 6 *
View data table for this chart

* Views captured on Cambridge Core between September 2016 - 8th March 2021. This data will be updated every 24 hours.

Send article to Kindle

To send this article to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about sending to your Kindle. Find out more about sending to your Kindle.

Note you can select to send to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be sent to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Inter Laboratory Comparison and Analysis on Mechanical Properties by Nanoindentation
Available formats
×

Send article to Dropbox

To send this article to your Dropbox account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Dropbox.

Inter Laboratory Comparison and Analysis on Mechanical Properties by Nanoindentation
Available formats
×

Send article to Google Drive

To send this article to your Google Drive account, please select one or more formats and confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your <service> account. Find out more about sending content to Google Drive.

Inter Laboratory Comparison and Analysis on Mechanical Properties by Nanoindentation
Available formats
×
×

Reply to: Submit a response


Your details


Conflicting interests

Do you have any conflicting interests? *